Embodiment 1
[0028] A heat-insulating curtain is woven from a chain thread, a weft insertion thread and a heat-insulating thread. figure 1 It is the digital map of lapped yarn of straight chain knitting line: 0-1 / 1-0 / / , knitting chain is a coil wale formed by lapping yarn on the same knitting needle all the time, and the knitting chain , there is no intersection between the longitudinal rows. figure 1 For open chains, insert a heat-insulating wire between two adjacent chains. It is also possible to set the open knitting chain as a closed knitting chain, and the lapping number of the closed knitting chain is 0-1 / / . Similarly, between two adjacent closed braided chains, a heat-insulating wire is inserted straight.
[0029] The knitting chain can also be set to a hexagonal curve, such as figure 2 As mentioned above, the lap yarn number is 0-1 / 1-0 / 0-1 / 1-2 / 1-2 / 2-1 / 1-0 / / , and a heat insulation line is set between two adjacent knitting chains , at this time, the insulation line is a curve, a...
Embodiment 2
[0034] This example is a method for preparing heat-insulating yarn. The yarn is treated with nano-titanium dioxide finishing agent on the warping machine. The warp reed, tension roller, static eliminator, finishing agent adder, yarn storage device, telescopic reed and yarn guide roller are evenly wound onto the warp beam. The nano-titanium dioxide finishing agent is stored in the finishing agent adder, and when the yarn passes through the finishing agent adder, the finishing agent is coated on the yarn as the roller rotates.
[0035] Among them, the preparation method of the nano-titanium dioxide finishing agent is: in deionized water, add 3% dodecylbenzenesulfonic acid, 5.0% graphene oxide, 5.0% nano-titanium dioxide powder, 8.0% resistant starch, and stir evenly Afterwards, disperse with ultrasound for 10-20 minutes.
[0036] In deionized water, add 3.0%~5.0% dodecylbenzenesulfonic acid, 5.0%~10.0% graphene oxide, 5.0%~15.0% nano titanium dioxide powder, 8.0%~15.0% resistan...
Embodiment 3
[0038] In this example, the preparation method of the nano-titanium dioxide finishing agent is to add 5.0% dodecylbenzenesulfonic acid, 10.0% graphene oxide, 15.0% nano-titanium dioxide powder, and 15.0% resistant starch in deionized water , after stirring evenly, disperse with ultrasound for 10~20min.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com