Device for improving interlayer bonding
A technology for improving layers and force-applying devices, applied in lamination devices, lamination, layered products, etc., can solve problems such as air bubbles, uneven distribution, and affecting bonding effects, so as to improve processing efficiency and promote reasonable and uniform distribution , Improve the effect of bonding effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0065] A device to improve interlayer bonding, such as figure 1 , figure 2 As shown, it includes an ultrasonic vibrator 11, a vibrator box 10, a force applying device and a vacuum bag.
[0066] The ultrasonic exciter 11 is placed in the exciter box 10, the exciter box 10 is provided with a sleeve on the top and bottom, and there are two force-applying devices, which are respectively connected to the exciter box 10 through two upper and lower sleeves , Two force-applying devices are set coaxially. The vacuum bag is connected with the vacuum pump 9 through the vacuum hole.
[0067] The force applying device includes a support plate 1 , a support frame and a screw rod 12 , and the screw rod 12 is provided with a rotating handle 6 , a first locking handle 5 and a second locking handle 7 .
Embodiment 2
[0069] This embodiment provides a device for improving interlayer bonding, and its structure is basically the same as that of the device for improving interlayer bonding provided in Example 1. The device in this embodiment can be placed vertically, or it can be Placed horizontally, the difference is that the vacuum unit 13 of this embodiment is a vacuum box, and there are four force-applying devices.
[0070] The exciter box 10 is provided with a sleeve respectively on the upper, lower, left, and right sides, and the screw rods 12 of the four force applying devices are respectively connected with the four sleeves. The vibrator box 10 is fixedly arranged at the center of the vacuum box.
Embodiment 3
[0072] A method for improving interlayer bonding, using the device of embodiment 1, comprising the following steps:
[0073] Step 1. Determine that the activation time of glue 17 is 50 minutes, and the maximum pressure that the insulation material layer can withstand is 0.5 MPa;
[0074] Step 2. After the thermal insulation material is bonded to the bulkhead through the glue 17 to prepare the composite material, the composite material, the force applying device and the ultrasonic exciter 11 are placed in the vacuum bag;
[0075] Step 3. According to the reading of the pressure sensor, adjust the rotating handle 6 and adjust the length of the screw. When the reading of the pressure sensor 2 is 0.35MPa, fix the first locking handle 5 and the second locking handle 7;
[0076] Step 4. Regulate the pressure in the vacuum unit 13 to negative pressure;
[0077] Step 5. Set the working time of the ultrasonic exciter 11 to 50 minutes, turn on the ultrasonic exciter 11 to work, and aut...