A preservative and anti-mildew technology, applied in the direction of wood treatment, wood impregnation, wood impregnation, etc., can solve the problems of loss, the effect is not lasting, the single function of anti-mildew preservatives, etc., to increase adhesion, excellent effect, and isolate external The effect of environmental impact
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] 1. Weigh 100 parts by weight of absolute ethanol under normal temperature and pressure, and add 1.1 parts by weight of 3-aminopropyltriethoxysilane to the base liquid as the base liquid of the metal-complex silicone gel hydrophobic fungicide Coupling agent and 0.17 parts by weight of copper chloride; Stir at a constant speed for 30 minutes; Continue to add 10 parts by weight of methyltriethoxysilane to stir; Then use glacial acetic acid to adjust the pH of the solution and stir for 2 hours to obtain mildew-proof and anti-corrosion agent.
[0034] 2. Put the prepared wood into a beaker with anti-mildew preservative and stir for 24 hours, then place it in the air to dry for 30 minutes; then soak the wood in the anti-mildew preservative for 5 minutes, air dry for 30 minutes, and cycle this step 5 times ; After drying the wood in an oven at 103°C for 24 hours, place it at room temperature for 3 days to obtain the wood treated with the anti-mold preservative.
[0035] The w...
Embodiment 2
[0037] 1. Weigh 120 parts by weight of dehydrated alcohol, as the base liquid of the metal-complex silicone gel hydrophobic type antifungal agent, add 1.3 parts by weight of 3-aminopropyltriethoxysilane coupling agent and 0.2 parts by weight of copper chloride, stirred at a constant speed for 30 minutes; continued to add 12 parts by weight of methyltriethoxysilane and stirred; then adjusted the pH of the solution to 4 with glacial acetic acid and stirred for 2 hours to obtain an anti-mold preservative.
[0038] 2. Put the prepared wood into a beaker with anti-mildew preservative, impregnate under vacuum pressure for 2 hours, stir at room temperature and pressure for 12 hours, then place it in the air to dry for 30 minutes; then impregnate the wood for 5 minutes, air dry for 30 minutes, and cycle This step is performed 5 times; the wood is dried in an oven at 103°C for 24 hours, and then placed at room temperature for 3 days to obtain the wood treated with the anti-mold preserva...
Embodiment 3
[0041] 1. Weigh 150 parts by weight of absolute ethanol as the base liquid of the metal-complex silicone gel hydrophobic fungicide. This is the base liquid of the preservative; add 1.3 parts by weight of 3-aminopropyltri Ethoxysilane coupling agent and 0.2 parts by weight of copper sulfate, stirring at a constant speed for 30 minutes; continue to add 15 parts by weight of methyltriethoxysilane and stir; then use dilute sulfuric acid to adjust the pH of the solution to 3 and stir for 2h, Made anti-mildew preservative.
[0042] 2. Put the prepared wood into a beaker with anti-mildew preservative and stir for 24 hours, then place it in the air to dry for 30 minutes; then impregnate the wood for 5 minutes, air dry for 30 minutes, and cycle this step 5 times; put the wood at 103°C After drying in an oven for 24 hours, place it at room temperature for 3 days to obtain the wood treated with the anti-mold preservative.
[0043] The wood treated with anti-mold preservative was charact...