[0025] A method for preparing a moisture-absorbing and quick-drying finishing agent for textiles, comprising the steps of:
[0026] (1) Add 2mol of allyl alcohol polyether in the reaction flask, the molecular weight of allyl alcohol polyether is 2000, drop 1mol of hydrogen-containing silicone oil into the reaction flask by means of a constant pressure burette, the molecular weight of hydrogen-containing silicone oil is 5600, Under the platinum catalyst, react at 80-90°C to prepare intermediate A;
[0027] (2) Add 2mol of allyl epoxy polyether and an appropriate amount of isopropanol solvent into the reaction flask, drop 1mol of hydrogen-containing silicone oil into the reaction flask with the help of a constant pressure burette, under the platinum catalyst, at 70-80 °C reaction to prepare intermediate B;
[0028] (3) Add 1 mol of intermediate B, 2 mol of polyetheramine ED2003 and an appropriate amount of isopropanol solvent into a reaction flask, and react at 70-80°C for 10-2...
Embodiment 2
[0031] A method for preparing a moisture-absorbing and quick-drying finishing agent for textiles, comprising the steps of:
[0032] (1) Add 2mol of allyl alcohol polyether in the reaction flask, the molecular weight of the allyl alcohol polyether is 1200, drop 1mol of hydrogen-containing silicone oil into the reaction flask by means of a constant pressure burette, the molecular weight of hydrogen-containing silicone oil is 4300, Under the platinum catalyst, react at 80-90°C to prepare intermediate A;
[0033] (2) Add 2mol of allyl epoxy polyether and an appropriate amount of isopropanol solvent into the reaction flask, drop 1mol of hydrogen-containing silicone oil into the reaction flask with the help of a constant pressure burette, under the platinum catalyst, at 70-80 °C reaction to prepare intermediate B;
[0034] (3) Add 1 mol of intermediate B, 2 mol of polyetheramine ED2003 and an appropriate amount of isopropanol solvent into a reaction flask, and react at 70-80°C for ...
Embodiment 3
[0037] A method for preparing a moisture-absorbing and quick-drying finishing agent for textiles, comprising the steps of:
[0038] (1) Add 2mol of allyl alcohol polyether in the reaction flask, the molecular weight of allyl alcohol polyether is 2500, drop 1mol of hydrogen-containing silicone oil into the reaction flask by means of a constant pressure burette, the molecular weight of hydrogen-containing silicone oil is 6600, Under the platinum catalyst, react at 80-90°C to prepare intermediate A;
[0039] (2) Add 2mol of allyl epoxy polyether and an appropriate amount of isopropanol solvent into the reaction flask, drop 1mol of hydrogen-containing silicone oil into the reaction flask with the help of a constant pressure burette, under the platinum catalyst, at 70-80 °C reaction to prepare intermediate B;
[0040] (3) Add 1 mol of intermediate B, 2 mol of polyetheramine ED2003 and an appropriate amount of isopropanol solvent into a reaction flask, and react at 70-80°C for 10-2...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com