Embodiment 1
[0037] like figure 1 As shown, the embodiment of the present invention provides a preparation method of a PHBV-silk fibroin slow-release film containing anti-fibrosis nanoparticles, comprising the following preparation steps:
[0038] S1. Extract silk fibroin and post-process silk fibroin: clean the surface of natural silkworm cocoons and cut them into pieces, add them to 0.02M NaCO3 solution; A. Heat and boil for 30 minutes; B. Discard the NaCO3 liquid and wash the silk with deionized water vegan fiber;
[0039] Repeat steps A and B 3 times to obtain silk fibroin fibers;
[0040] For post-treatment of silk fibroin fiber, add silk fibroin to 9.3M LiBr solution to obtain 25% (w / v%) silk fibroin-LiBr solution, heat in a water bath at 60°C for 4 hours, and dissolve the mixed solution after the silk fibroin fiber is completely dissolved Put it into a dialysis bag, dialyze in deionized water for 3 days, replace the deionized water every 8 hours, centrifuge the solution after dial...
Embodiment 2
[0047] like figure 1 As shown, the embodiment of the present invention provides a preparation method of a PHBV-silk fibroin slow-release film containing anti-fibrosis nanoparticles, comprising the following preparation steps:
[0048] S1. Extract silk fibroin and post-process silk fibroin: clean the surface of natural silkworm cocoons and cut them into pieces, add them to 0.02M NaCO3 solution; A. Heat and boil for 30 minutes; B. Discard the NaCO3 liquid and wash the silk with deionized water vegan fiber;
[0049] Repeat steps A and B 3 times to obtain silk fibroin fibers;
[0050] For post-treatment of silk fibroin fiber, add silk fibroin to 9.3M LiBr solution to obtain 25% (w / v%) silk fibroin-LiBr solution, heat in a water bath at 60°C for 4 hours, and dissolve the mixed solution after the silk fibroin fiber is completely dissolved Put it into a dialysis bag, dialyze in deionized water for 3 days, replace the deionized water every 8 hours, centrifuge the solution after dial...
experiment example
[0057] The PHBV-silk fibroin film containing drug-loaded nanoparticles proposed by the present invention and pure PHBV, PHBV-silk fibroin, and the PHBV film containing drug-loaded nanoparticles are observed with a scanning electron microscope, and the observation results (see figure 2 );
[0058] Finally, it is found that the performance of the PHBV-silk fibroin film containing drug-loaded nanoparticles proposed by the present invention is significantly better than that of pure PHBV, PHBV-silk fibroin, and PHBV films containing drug-loaded nanoparticles.