An amino acid, coating technology, applied in the application, additional food elements, animal feed and other directions, can solve the problems of inability to adjust the reasonable range, limited use effect, fast absorption speed, etc., to improve the coating effect, improve utilization efficiency, reduce Dissolution effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] This embodiment provides a coated amino acid, a coated crystalline amino acid and a coating agent, wherein the coating agent is a combination of myristic acid and rice protein, and the crystalline amino acid is a combination of methionine, arginine and phenylalanine. Crystalline amino acids are powders.
[0027] In terms of weight percentage, the coated amino acid in this embodiment includes the following components:
[0028]
[0029]
[0030] The preparation method of coated amino acid in this embodiment comprises the following steps:
[0031] Weigh each component according to the formula, heat myristic acid to 55°C to dissolve, then add rice protein, methionine, arginine and phenylalanine to disperse, and spray dry to obtain coated amino acid.
[0032] The air inlet temperature of the spray drying is 30°C, and the air outlet temperature is 25°C; the pressure of the spray drying is about 5MPa, and the spray speed is about 10L / min.
Embodiment 2
[0034] This embodiment provides a coated amino acid, coated crystalline amino acid, coating agent and guar gum, wherein the coating agent is a combination of myristic acid and rice protein, and the crystalline amino acid is methionine, arginine and phenylalanine A combination of acids, all crystalline amino acids are powders.
[0035] In terms of weight percentage, the coated amino acid in this embodiment includes the following components:
[0036]
[0037] The preparation method of coated amino acid in this embodiment comprises the following steps:
[0038] Weigh each component according to the formula, heat myristic acid to 55°C to dissolve, add rice protein, guar gum, methionine, arginine and phenylalanine to disperse, and spray dry to obtain a coating amino acid.
[0039] The air inlet temperature of the spray drying is 30°C, and the air outlet temperature is 25°C; the pressure of the spray drying is about 5MPa, and the spray speed is about 10L / min.
Embodiment 3
[0041] This embodiment provides a coated amino acid, coated crystalline amino acid, coating agent and guar gum, wherein the coating agent is a combination of lauric acid and rice protein, and the crystalline amino acid is methionine, arginine and phenylalanine Combination, all crystal amino acids used are powder.
[0042] In terms of weight percentage, the coated amino acid in this embodiment includes the following components:
[0043]
[0044] The preparation method of coated amino acid in this embodiment comprises the following steps:
[0045] Weigh each component according to the formula, heat lauric acid to 50°C to dissolve, then add rice protein, guar gum, methionine, arginine and phenylalanine to disperse, and spray dry to obtain coated amino acid .
[0046] The air inlet temperature of the spray drying is 30°C, and the air outlet temperature is 25°C; the pressure of the spray drying is about 5MPa, and the spray speed is about 10L / min.