Pure natural deodorant high-ductility ultra-thin overlay asphalt mixture modifier
A technology of asphalt mixture and modifier, which is applied in the field of high-elongation elastic ultra-thin overlay asphalt mixture modifier, which can solve the problems of odor at the pavement drain, affecting human health and traffic environment, etc., and achieves improvement Asphalt rheological properties, good for health, simple and reliable operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] The present invention is a pure natural odor-removing high-elongation elastic ultra-thin overlay asphalt mixture modifier, comprising the following components in parts by weight: 58 parts of thermoplastic elastomer materials, 30 parts of polyvinyl butyral, 2 parts of p-tert-butylphenol formaldehyde resin, 2 parts of chloropropane resin ethylene-propylene copolymer, 5 parts of polymer organic wax, 3 parts of asphalt recycled material, 3 parts of citric acid, 3 parts of malic acid, 4 parts of thymol, 16 parts of Moutan bark extract, 20 parts of peppermint extract, 14 parts of woody extract, 12 parts of camellia extract, 6 parts of methylparaben, 5 parts of propylparaben, 97 parts of water;
[0026] The high-elongation elastic ultra-thin overlay asphalt mixture modifier of this pure natural deodorization is prepared by the following steps:
[0027] Step 1: heating the thermoplastic elastomer material to 155-165° C., adding the polyvinyl butyral, and reacting for 20-60 minu...
Embodiment 2
[0045] The implementation mode of this example is basically the same as that of Example 1, the difference is that the pure natural odor-removing high-elongation elastic ultra-thin overlay asphalt mixture modifier includes the following components in parts by weight: thermoplastic elastomer material 58 30 parts of polyvinyl butyral, 2 parts of p-tert-butylphenol formaldehyde resin, 2 parts of ethylene-propylene copolymer of chloropropene resin, 5 parts of polymer organic wax, 3 parts of asphalt recycled material, 7 parts of citric acid, 7 parts of malic acid, 8 parts of thymol, 22 parts of Moutan bark extract, 27 parts of mint extract, 19 parts of woody extract, 17 parts of camellia extract, 1 part of methylparaben, propylparaben 1 part, 88 parts of water.
Embodiment 3
[0047] The implementation mode of this example is basically the same as that of Example 1, the difference is that the multi-energy-efficiency thin-layer modifier of the high-elongation elastic ultra-thin overlay asphalt mixture includes the following components in parts by weight: thermoplastic elastomer material 58 30 parts of polyvinyl butyral, 4 parts of p-tert-butylphenol formaldehyde resin, 4 parts of ethylene-propylene copolymer of chloropropane resin, 8 parts of polymer organic wax, and 5 parts of asphalt recycled material.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com