A copper anode slime and rapid determination technology, which is applied in the field of metallurgy, can solve problems such as difficulty in ensuring the accuracy of analysis results, detection limits of analysis and detection methods and matrix interference with precious metal element analysis, and inability to meet the production control and metal balance needs of precious metal elements, etc. , to achieve the effect of improving the timeliness of analysis and simplifying the operation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] (1) Sample treatment, mix 5.0 mL of copper anode slime leaching solution with 5.0 mL of aqua regia and put it into a beaker with a capacity of 200 mL and heat it with an electric hot plate to make it evaporate to a volume of about 2-3 mL. Gold, palladium, platinum and other coexisting elements are completely dissolved. The cooled solution is placed in a 100mL volumetric flask A, and the volume is adjusted with water. Then, 5.0mL of the solution is removed from the volumetric flask A and placed in a 100mL volumetric flask B. The beaker needs to be rinsed with hydrochloric acid before use to avoid contamination.
[0017] From the analysis of the whole analysis process, although the mass spectrometry is more suitable for the nitric acid medium, the precious metal elements are the most stable in the hydrochloric acid medium. The whole experimental process also confirms this, so the hydrochloric acid medium is determined.
[0018] (2) Select the standard solution, select 200...
Embodiment 2
[0023] (1) Sample treatment, mix 5.0 mL of copper anode slime leaching solution with 5.0 mL of aqua regia and put it into a beaker with a capacity of 200 mL and heat it with an electric hot plate to make it evaporate to a volume of about 2-3 mL. Gold, palladium, platinum and other coexisting elements are completely dissolved. The cooled solution is placed in a 100mL volumetric flask A, and the volume is adjusted with water. Then, 5.0mL of the solution is removed from the volumetric flask A and placed in a 100mL volumetric flask B. The beaker needs to be rinsed with hydrochloric acid before use to avoid contamination.
[0024] (2) Select the standard solution, select 200 mL of the reference solution, and the density of gold, palladium and platinum in the reference solution is 50 μg / L, respectively. In a 500 mL volumetric flask, dilute to volume with hydrochloric acid to obtain a first-level mixed solution, then pipette 10.0 mL of the first-level mixed solution into a 200-mL vol...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com