Embodiment 1
[0018] Embodiment 1: prepare firebrick with waste cloth
[0019] 1.1 Compounding Commercially available ammonium polyphosphate, pentaerythritol, melamine and expandable graphite powder are mixed in proportion to prepare a high-efficiency flame retardant, so that the content of N, P and C (percentage by weight) is N: 7%, P: 8%, C: 8%. Prepare 2Kg of high-efficiency flame retardant. Mix 6Kg of commercially available phenolic resin with a high-efficiency flame retardant, process it into powder, add 2Kg of water, and stir evenly to form a gel.
[0020] 1.2 Preparation of fire-resistant bricks Cut up 10Kg of leftover materials received from the garment factory, mix them with the above-mentioned glue in a weight ratio of 1:1, put them into the brick making machine to make fire-resistant bricks, and dry them in the air That's it. Can be used as a partition wall.
Embodiment 2
[0021] Embodiment 2: Prepare trapezoidal fire-resistant block with waste cloth
[0022] 2.1 Compounding Commercially available ammonium polyphosphate, pentaerythritol, melamine and expandable graphite powder are mixed in proportion to prepare a high-efficiency flame retardant, so that the content of N, P and C (percentage by weight) is N: 8%, P: 5%, C: 8%. Prepare 3Kg of high-efficiency flame retardant. Mix 3.5Kg of commercially available phenolic resin with a high-efficiency flame retardant, process it into powder, add 3.5Kg of water, and stir evenly to form a gel.
[0023] 2.2 Preparation of fire-resistant bricks. Cut up 10Kg of leftover materials collected from the garment factory, mix them with the above-mentioned glue in a weight ratio of 1:1, put them into a trapezoidal mold to make trapezoidal fire-resistant blocks, and dry them in the air. That's it. Can be used to block trapezoidal openings, or corners of walls.
Embodiment 3
[0024] Embodiment 3: Prepare fire-resistant brick with straw
[0025] 3.1 Compounding commercially available ammonium polyphosphate, pentaerythritol, melamine and expandable graphite powder, mixed in proportion to prepare a high-efficiency flame retardant, so that the content of N, P, and C (percentage by weight) is N: 7%, P: 10 %, C: 5%. Prepare 2Kg of high-efficiency flame retardant. Mix 4Kg of commercially available phenolic resin with a high-efficiency flame retardant, process it into powder, add 4Kg of water, and stir evenly to form a gel.
[0026] 3.2 Preparation of fire-resistant bricks: Chopped 9Kg of straw, mixed evenly with the above-mentioned glue in a weight ratio of 0.9:1, put it into the brick making machine to make fire-resistant bricks, and dried them in the air.