Cellulose material possessing dethiol action and its preparation method
A technology for cellulose and desulfurization, applied in separation methods, refining with metal salts, chemical instruments and methods, etc., can solve the problems of waste lye pollution, complicated processes, high cost, and achieve high safety, wide applicability, Easy to use effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0019] The preparation method of carboxymethyl cellulose copper and carboxyethyl cellulose copper is as follows: according to the molar ratio of copper ion and sodium ion is 0.5-2.5, carboxymethyl cellulose sodium, carboxyethyl cellulose sodium and copper salt are mixed in Fully mixed and reacted under solid conditions, and added water accounting for 0-10% of the total material weight, washed with water to remove water-soluble matter after the reaction, and dried naturally to obtain corresponding sweetening materials copper carboxymethyl cellulose and copper carboxyethyl cellulose.
[0020] Copper carboxymethyl cellulose and copper carboxyethyl cellulose mixed materials are obtained by the following two methods:
[0021] Method 1: directly mix the prepared copper carboxymethyl cellulose and copper carboxyethyl cellulose;
[0022] Method 2: According to the molar ratio of copper ion and sodium ion being 0.5-2.5, the mixture of sodium carboxymethylcellulose and sodium carboxyeth...
Embodiment 1
[0034] Take 10.0 grams of sodium carboxymethyl cellulose and 26.2 grams of copper chloride, and mix them thoroughly for 10 minutes under stirring. During the mixing process, spray water mist to wet the mixture. The total amount of water sprayed is 1.5 grams, and continue to stir for 5 minutes. Washed twice with water and dried naturally to obtain sweetened material M1.
Embodiment 2
[0036] Take 10.0 g of sodium carboxymethyl cellulose and 48.9 g of copper sulfate pentahydrate, mix them thoroughly for 10 minutes under high-speed stirring, wash the mixture twice with 200 ml of water, and dry naturally to obtain sweetened material M2.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com