Corrosion-resistant welding rod and preparing method thereof
A corrosion-resistant, welding rod technology, applied in welding equipment, welding media, manufacturing tools, etc., can solve problems such as narrow application range, component failure, and not widely used, and achieve the effects of wide application, improved toughness, and good welding performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0013] The preparation method of welding rod is as follows:
[0014] A. Weigh the coating components in the following percentages by weight and mix:
[0015] Tungsten carbide 2~10%, boron carbide or boron nitride 2~8%, nickel powder 2~10%, copper 0.30~0.85%, rare earth 0.2~4.60%, manganese nitrogen alloy and / or vanadium nitrogen alloy any proportion 0.20~ 2.80%, ferromolybdenum 0.6-3.2%, marble 25-38%, titanium dioxide 2-8%, fluorite 1-6%, ferromanganese 3-8%, ferro-vanadium 0.35-4%, ferro-niobium or ferro-titanium 0.35 ~4%, ferrochrome balance, wherein, the ferromanganese is low-carbon ferromanganese or micro-carbon ferromanganese, and the ferrochrome is low-carbon ferrochrome or micro-carbon ferrochrome; the particle size of each component of the coating is 80-200 mesh ;
[0016] B, add the sodium bicarbonate that accounts for 4~6% of mixed component gross weight in the mixed component that step A gains, bond with sodium water glass;
Embodiment 1
[0031] The raw material formula of the coating is (the sum of weight percentages is 100%): 2% tungsten carbide, 3% boron carbide, 4% nickel powder, 0.40% copper, 1.60% rare earth, manganese nitrogen alloy and / or vanadium nitrogen alloy in any proportion 0.40 %, 0.8% ferromolybdenum, 28% marble, 4% titanium dioxide, 5% fluorite, 4% low-carbon ferromanganese, 0.45% ferro-vanadium, 0.35% ferro-titanium, and the balance of low-carbon ferrochrome.
[0032] Then make welding rods according to the above method, the hardness of the surfacing layer is ≥ HRC55, and the corrosion rate is 0.008 mm / year (the corrosion rate is less than 0.05 mm / year, the metal The corrosion resistance is excellent; the corrosion rate is 0.05-0.5 mm / year, the corrosion resistance of the metal is considered good), the wear resistance is good, and the corrosion resistance is good.
Embodiment 2
[0034] The raw material formula of the coating is (the sum of weight percentages is 100%): tungsten carbide 8%, boron carbide 6%, nickel powder 6%, copper 0.60%, rare earth 2.60%, manganese nitrogen alloy and / or vanadium nitrogen alloy in any proportion 2.0 %, 2.0% ferromolybdenum, 30% marble, 6% titanium dioxide, 5% fluorite, 5% low-carbon ferromanganese, 2% ferro-vanadium, 3% ferro-titanium, and the balance of low-carbon ferrochrome.
[0035] Then make welding rods according to the above method, the hardness of the surfacing layer is ≥HRC60, and the corrosion rate is 0.045 mm / year in the sodium bicarbonate solution with a concentration of 30% at a temperature of 25oC (the corrosion rate is less than 0.05 mm / year, The corrosion resistance is excellent; the corrosion rate is 0.05-0.5 mm / year, the corrosion resistance of the metal is considered good), the wear resistance is very good, and the corrosion resistance is good.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
corrosion rate | aaaaa | aaaaa |
corrosion rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com