All case nanometer high energy composite ceramic and its preparation method
A nano-composite, ceramic technology, applied in the field of ceramics, can solve problems such as being unsuitable for rapid and effective production, unable to achieve health care effects, and lack of health care functions, and achieve the effects of improving blood supply and oxygen supply, accelerating repair, and relieving pain.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A nanocomposite ceramic, which uses volcanic rock and tourmaline powder as main raw materials, and is characterized in that the components according to weight percentage include: 10-20% of volcanic rock, 30-50% of tourmaline powder, 2-8% of ruby powder, and 3-10% of kaolin %, Datong soil 2-10%, spodumene 2-10% and albite 4-20%.
[0018] The tourmaline powder is lithium tourmaline powder, or iron tourmaline powder, or magnesium tourmaline powder, or a mixed powder of the three.
[0019] A preparation method of nanocomposite ceramics, characterized in that it comprises the following steps:
[0020] A. First crush and grind the tourmaline until the particle size is 30-80nm;
[0021] B. Crush and sieve volcanic rock and tourmaline, mix and stir with 2-6% by weight binder in proportion, granulate, dry, and then fire for 8-12 hours at a temperature of 800-1200°C. Cool and pulverize for later use;
[0022] C, ruby, kaolin, Datong soil, spodumene and albite are crushed and...
Embodiment 2
[0026] A nano-composite ceramic, with volcanic rock and tourmaline powder as main raw materials, characterized in that the components according to weight percentage include: 20% of volcanic rock, 40% of tourmaline powder, 5% of ruby powder, 7% of kaolin, 5% of Datong soil, lithium Pyroxene 8% and albite 15%.
[0027] The tourmaline powder is a mixed powder of lithium tourmaline powder, iron tourmaline powder and magnesium tourmaline powder.
[0028] A preparation method of nanocomposite ceramics, characterized in that it comprises the following steps:
[0029] A. First crush and grind the tourmaline until the particle size is 30-80nm;
[0030] B. Crush and sieve volcanic rock and tourmaline, mix and stir with 2 to 6% binder in proportion by weight, granulate, dry, and then fire for 8 to 12 hours. The temperature should reach 820°C, and finally cool and crush reserve;
[0031] C, ruby, kaolin, Datong soil, spodumene and albite are crushed and sieved, and then calcined into...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com