Paper disc type mosquito-repellent incense and method for preparing the same
A disc-type mosquito-repellent incense and paper-based technology, applied in botany equipment and methods, chemicals for biological control, animal repellents, etc., can solve the problems of easy extinguishment, unsuitable for large-scale production, etc., and achieve flammability Good, light weight, high production capacity effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] The waste paper raw materials are picked to remove large impurities, and the pulp is fully washed to remove fine impurities after deflaking, mainly to remove various rubber fillers and plastic sheets and other impurities in the waste paper pulp. If these are mixed in the pulp, it will affect the burning time of the product, or even cause flameout. Then, the concentration of the slurry entering the refiner should be controlled to be no less than 5%, and the slurry is entered into the refiner for refining. The beating degree of the slurry reaches about 32, and the waste paper fiber slurry is obtained.
[0031] Reasonable proportioning of raw materials, calculated by weight percentage, including 55% waste paper fiber, 35% charcoal powder, 5% plant fiber, and 5% starch, mixed and refined, and the thickness of the paperboard made is 3-3.2mm, pressed and dehydrated. Then punch it into a square or round mosquito coil with a mold. When the length reaches 1300mm, the ignition ti...
Embodiment 2
[0033] Waste paper fiber slurry is prepared by the method of Example 1, and then the raw materials are reasonably proportioned, by weight percentage, wherein waste paper fiber 50%, charcoal powder 35%, plant fiber 10%, starch 5%, mixed pulping . The thickness of the copied cardboard is 2.8-3mm. Squeeze and dehydrate, and then use a mold to press into square or round mosquito coils. When the length reaches 1400mm, the ignition time is more than 8 hours and 20 minutes, the flame will not be turned off, and the smoke will be small.
Embodiment 3
[0035] Waste paper fiber slurry is prepared by the method of Example 1, and then the raw materials are reasonably proportioned, by weight percentage, wherein 45% of waste paper fiber, 38% of charcoal powder, 12% of fiber in plants, 5% of starch, and mixed pulp . The thickness of the copied cardboard is 2.5-2.8mm. Squeeze and dehydrate, and then use a mold to press into square or round mosquito coils. When the length reaches 1450m, the ignition time is more than 8 hours and 40 minutes, the flame will not be turned off, and the smoke will be small.