Environmental protection type paint technique of furniture
An environmentally friendly paint and process technology, which is applied to the surface coating liquid device, pretreatment surface, coating, etc., can solve the problems of low hardness of the decorative surface, pollute the environment, endanger human health, etc., and achieve beautiful appearance and environmental protection. Pollution, low cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Embodiment 1, described paint process comprises the steps:
[0017] A, the white embryo is ground with a sandpaper grinder;
[0018] B. Criticize the polished board with dust to increase the smoothness of the surface;
[0019] C. Filling colorant or transparent putty;
[0020] D. Spray a high-hardness primer once;
[0021] E. Then grind again, clean up the excess ash, and grind the plate until it is smooth;
[0022] F. Spray polyurethane primer on the ground board to seal the paint surface of the board;
[0023] G. After two times of primer spraying and grinding, spray a new environmentally friendly topcoat for coloring;
[0024] H. Send the plate to a special ultraviolet drying line for drying and curing, and the drying time is 5 minutes.
[0025] The finish paint of the present invention is acrylic acid, which is a white liquid. When in use, a blending agent needs to be added for blending. Its weight ratio is the main agent: blending agent=2: 1, and the solid con...
Embodiment 2
[0026] Embodiment 2, this paint process comprises the steps:
[0027] A, the white embryo is ground with a sandpaper grinder;
[0028] B. Criticize the polished board with dust to increase the smoothness of the surface;
[0029] C. Filling colorant or transparent putty;
[0030] D. Spray a high-hardness primer once;
[0031] E. Then grind again, clean up the excess ash, and grind the plate until it is smooth;
[0032] F. Spray polyurethane primer on the ground board to seal the paint surface of the board;
[0033] G. After two times of primer spraying and grinding, spray a new environmentally friendly topcoat for coloring;
[0034] H. Send the plate into a special ultraviolet drying line for drying and curing, and the drying time is 10 minutes.
[0035] The finish paint of the present invention is acrylic acid, which is a white liquid. When in use, a blending agent needs to be added for blending. Its weight ratio is the main agent: blending agent=2: 1, and the solid conte...
Embodiment 3
[0036] Embodiment 3, paint process of the present invention comprises the steps:
[0037] A, the white embryo is ground with a sandpaper grinder;
[0038] B. Criticize the polished board with dust to increase the smoothness of the surface;
[0039] C. Filling colorant or transparent putty;
[0040] D. Spray a high-hardness primer once;
[0041] E. Then grind again, clean up the excess ash, and grind the plate until it is smooth;
[0042] F. Spray polyurethane primer on the ground board to seal the paint surface of the board;
[0043] G. After two times of primer spraying and grinding, spray a new environmentally friendly topcoat for coloring;
[0044] H. Send the plate to a special ultraviolet drying line for drying and curing, and the drying time is 20 minutes.
[0045] The finish paint of the present invention is acrylic acid, which is a white liquid. When in use, a blending agent needs to be added for blending. Its weight ratio is the main agent: blending agent=2: 1, a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com