Preparation method of charge positive charge filter material and application thereof
A technology of filter material and positive charge, applied in filtration and separation, separation methods, chemical instruments and methods, etc., can solve the problems of high cost, high manufacturing cost, unsuitable for wide application, etc., and achieve low cost and low cost of wastewater treatment , the effect of easy reprocessing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] To prepare a positive charge coating solution:
[0020] (1) Weigh 3g of polyvinyl alcohol; water, 97g; adjust the conductivity of the water at about 200μs, and the temperature at about 90°C;
[0021] (2) Put water into the container, then slowly add the weighed polyvinyl alcohol while stirring, and continue stirring for 10 minutes to prepare a positively charged coating solution.
[0022] The preparation method of described positively charged filter material comprises the steps:
[0023] Material selection and cleaning treatment: select old cotton cloth, wool, hemp, chemical fiber, etc. that meet the requirements, and carry out washing, decolorization, expansion and crushing treatment, control the length of the fiber to no more than 20cm, and then wash it with water, and set it aside;
[0024] Soaking and charging: Soak the processed raw materials in the above prepared positive charge coating solution, the liquid level of the coating solution is about 5cm above the upp...
Embodiment 2
[0028] To prepare a positive charge coating solution:
[0029] (1) Take chitosan polymer 5g; Water 95g; Regulate the conductivity of water at about 200μs, and the temperature at about 40°C;
[0030] (2) Put water into the container, then slowly put in the weighed chitosan polymer while stirring, and continue stirring for 10 minutes to prepare a positively charged coating solution.
[0031] The preparation method of described positively charged filter material comprises the steps:
[0032] Material selection and cleaning treatment: select the waste cotton cloth that meets the requirements, carry out crushing treatment, control the fiber length not to exceed 20cm, then wash it with water, and set it aside;
[0033] Soaking and charging: Soak the treated raw materials in the positively charged coating solution prepared above. The liquid level of the coating solution is about 5cm higher than the upper surface of the raw materials. Add 1% quaternary ammonium salt cross-linking age...
PUM