A technology for medical supplies and gels, applied in the field of gel medical supplies and their preparation, can solve the problems of difficulty in bathing patients with clean water, lack of medical supplies, etc., and achieves the effect of strengthening local skin immunity, enhancing metabolism, and removing dirt and cleaning effects. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0059] Prepare the gel of the gel medical article that total weight is 1000 grams and prevent decubitus ulcers:
[0060] In the first step, dissolve 0.5 grams of 2,4,4'-trichloro-2'-hydroxydiphenyl ether and 1 gram of vitamin E in 50 grams of glycerol, and let stand for 12 hours;
[0061] In the second step, 5 grams of cross-linked polyacrylic resin and 5 grams of hydroxyethyl cellulose are dissolved in 250 grams of distilled water to obtain a mixed solution of cross-linked polyacrylic resin and hydroxyethyl cellulose;
[0062] The 3rd step, 50 grams of hydroxypropyl chitosan, 10 grams of triethanolamine and 5 grams of sodium triethyldiamine tetraacetate are dissolved in 200 grams of distilled water;
[0063] In the fourth step, the glycerin solution containing 2,4,4'-trichloro-2'-hydroxyl diphenyl ether and vitamin E obtained in the first step is added into the cross-linked polymer obtained in the second step under stirring. In the mixed solution of acrylic resin and hydroxy...
Embodiment 2
[0082] Prepare the gel of the gel medical supplies for the treatment of decubitus with a total weight of 1000 grams:
[0083] In the first step, 2 grams of 2,4,4'-trichloro-2'-hydroxydiphenyl ether and 2 grams of vitamin C were dissolved in 10 grams of glycerol and 20 grams of propylene glycol, and allowed to stand for 10 hours;
[0084] In the second step, 10 grams of cross-linked polyacrylic resin and 5 grams of hydroxypropyl cellulose are dissolved in 350 grams of distilled water to obtain a mixed solution of cross-linked polyacrylic resin and hydroxypropyl cellulose;
[0085] The 3rd step, 30 gram carboxymethyl chitosan, 1 gram triethyl diamine tetraacetate potassium and 5 gram triethanolamine are dissolved in 300 gram distilled water;
[0086] In the fourth step, the glycerol solution containing 2,4,4'-trichloro-2'-hydroxyl diphenyl ether and vitamin C obtained in the first step is added to the cross-linked polystyrene obtained in the second step under stirring. In the m...
Embodiment 3
[0105] Prepare the gel of the gel medical article that total weight is 1000 grams and prevent decubitus ulcers:
[0106] In the first step, 5 grams of polyhexamethylene biguanide and 1.5 grams of lanolin were dissolved in 100 grams of distilled water and allowed to stand for 12 hours;
[0107] In the second step, 10 grams of cross-linked polyacrylic resin and 5 grams of hydroxyethyl cellulose are dissolved in 250 grams of distilled water to obtain a mixed solution of cross-linked polyacrylic resin and hydroxyethyl cellulose;
[0108] The 3rd step, 50 gram N-trimethyl chitosan oxides, 3 gram sodium citrate and 10 gram triethanolamine are dissolved in 300 gram distilled water;
[0109] In the fourth step, the glycerol solution containing 2,4,4'-trichloro-2'-hydroxyl diphenyl ether and lanolin obtained in the first step is added into the cross-linked polymer obtained in the second step under stirring. In the mixed solution of acrylic resin and hydroxyethyl cellulose, continue to...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com