Method for producing superconducting carbon black with high specific surface area

A technology of superconducting carbon black and high specific surface area, applied in sustainable manufacturing/processing, climate sustainability, chemical industry, etc., can solve the problems of large equipment investment and long process, and achieve small equipment investment and stable product performance , the effect of increasing strength

Active Publication Date: 2011-09-07
山西永东化工股份有限公司
View PDF6 Cites 31 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, the production technology of superconducting carbon black in China is not yet mature. Foreign superconducting carbon black is produced by a two-step method. First, it is made into basic carbon black, and then it is made into superconducting carbon black by high temperature heat treatment. The process is long and the investment in equipment is large.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0013] Using the oil furnace method, in the first section of the ultra-high temperature carbon black reaction furnace with an effective size of 12000χ1500χ1100, the gas flow rate is 55-125m / s, and the air flow rate is 100-320m 3 / h, high-temperature carbon black flue gas at 1900-2200°C is produced by complete combustion; in the second throat section, methane, ethylene, acetylene, etc. in the high-temperature gas are fully mixed with the raw material oil injected into the throat to form thermal oxidation Critical state.

[0014] The raw material oil is light coal tar, which is composed of three products: light oil, decrystallized washing oil and decrystallized anthracene oil in a mass ratio of 2:5:3. The feed rate of light coal tar is 72kg / h. Composition of tar: 13.1% of benzene, 6.9% of toluene, 50.5% of decrystallized washing oil, and 29.5% of decrystallized anthracene oil.

[0015] Mix with the gas from the combustion section, add K2CO3 catalyst in the reaction section acco...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
particle diameteraaaaaaaaaa
adsorption capacityaaaaaaaaaa
particle diameteraaaaaaaaaa
Login to view more

Abstract

The invention relates to a method for producing superconducting carbon black with high specific surface area, and aims to make a production process simple and product performance stable. The method comprises the following steps of: completely combusting gas in a combustion section of a reaction furnace, mixing the gas, air and raw oil, adding into a throat pipe section of the reaction furnace, and making the temperature of a reaction section of the reaction furnace reach 1,300 to 1,600 DEG C under the action of a K2CO3 catalyst; performing thermal cracking and thermal polycondensation on the gas and the raw oil rapidly to generate the superconducting carbon black; continuously reacting the superconducting carbon black with a CO2 catalyst in a rapid cooling section of the reaction furnace,and performing catalytic activation on the superconducting carbon black to form a developed pore structure and improve the specific surface area of the superconducting carbon black; exchanging the flue gas of the superconducting carbon black with cold air by using an air preheater in a retention section of the reaction furnace to reduce the temperature to be lower than 600 DEG C; and when reaction for preparing a product from raw materials is finished, cooling the superconducting carbon black to 320-350 DEG C by using a tubular rapid cooling boiler, slowly cooling, adding into a bag filter, and collecting, wherein recycled heat is used for generating electricity.

Description

technical field [0001] The invention specifically relates to a production method of superconducting carbon black with high specific surface area. Background technique [0002] High specific surface area superconductive carbon black can reduce the usage of general carbon black and conductive carbon black, and significantly enhance the performance of materials. In terms of superconducting carbon black used in new energy, Chinese invention patent 200710144767.1 adopts vibration method to add XC-72 or BP2000 superconducting carbon black to PTFE, make carbon paper under the action of catalyst, etc., and then make proton exchange membrane fuel cell electrodes. Its XC-72 or BP2000 superconducting carbon black is a product of Cabot Corporation of the United States. In Chinese invention patent 201010240465.6, nano-scale superconductive carbon black is used as the negative electrode active material additive of lead-acid batteries, and the service life of ordinary lead-acid batteries...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09C1/50
CPCY02P20/10
Inventor 刘东良焉福林周华忠张巍刘东杰刘东玉贺乐斌周霞萍
Owner 山西永东化工股份有限公司
Who we serve
  • R&D Engineer