An anti-counterfeiting ink and pigment technology, applied in inks, household appliances, applications, etc., can solve the problems of large amount of ink raw materials, difficult to remove odor, high ink solid content, environmental protection and health protection, good printing effect, good dispersibility sexual effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0048] The present invention also provides a preparation method of anti-counterfeiting ink, comprising:
[0049] a) dissolving the water-based polyacrylic acid resin in a solvent to obtain a binder solution;
[0050] b) mixing the binder solution with the pigment and dispersing evenly;
[0051] c) adding a filler, a leveling agent, and a wetting agent to the solution obtained in the step b) in sequence, and performing an emulsification operation to obtain an anti-counterfeiting ink.
[0052] According to the present invention, the raw materials are calculated by weight fraction: 10-40 parts of pigment; 30-60 parts of water-based vehicle; 0.1-5 parts of leveling agent; 0.1-5 parts of wetting agent; wherein the pigment is matte powder; The water-based binder is water-based polyacrylic resin; the solid content of the anti-counterfeiting ink is 30wt%-60wt%. Preferably, the pigment is 15-35 parts; the water-based vehicle is 40-50 parts; the leveling agent is 0.3-3 parts; the wett...
Embodiment 1
[0057] Prepare materials according to the following weight ratio: matte powder 10g; water-based polyacrylic resin 30g; pearl powder 5g, C 3 h 8 N 2 O0.3g; wetting agent 0.3g, defoamer 0.5g; water 5g, ethanol 10g.
[0058] In the light-shielding and dust-free workshop, the temperature is 25°C, and the humidity is 65%. In the reaction kettle, put solvent water and ethanol first, then put in water-based polyacrylic resin, soak for 2 hours, stir for 45 minutes, and add the pigment after it is completely dissolved. Disperse at 2500rad / min for 30 minutes, then add pearl powder to stir evenly, then add leveling agent, wetting agent and defoamer in turn, and emulsify for 45 minutes. The speed of emulsifier is 2500rad / min. ink. After the ink is ready, check the hue and control the viscosity at 50S. Use a No. 3 Zahn cup to test, and the solid content is 30%. After passing the test, filter it with a 200-mesh filter cloth, and pack it in a plastic barrel for storage.
Embodiment 2
[0060] Prepare materials according to the following weight ratio: matte powder 40g, water-based polyacrylic resin 60g, pearl powder 10g, C 3 h 8 N 2 O3g, wetting agent 3g, defoamer 3g, water 10g, ethanol 20g.
[0061] In the light-shielding and dust-free workshop, the temperature is 27°C, and the humidity is 70%. In the reaction kettle, put solvent water and ethanol first, then put in water-based polyacrylic resin, soak for 2.5 hours, stir for 45 minutes, and add the pigment after it is completely dissolved. Disperse at 2500rad / min for 30 minutes, add pearlescent powder to stir evenly, then add leveling agent, wetting agent and defoamer in turn, emulsify at 2500rad / min for 45 minutes, after the ink is ready, check the hue and control the viscosity at 50-80S, tested with No. 3 Zahn Cup, the solid content is 60%, filtered with 200-mesh filter cloth after passing the test, and packed in plastic barrels for storage.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com