[0014] 200 kg of water, 3 kg of hydroxyethyl cellulose, 4 kg of dispersant, 1.5 kg of defoamer, 1.5 kg of bactericide, 20 kg of antifreeze, 1 kg of regulator, 60 kg of calcium carbonate, 40 kg of titanium dioxide, quartz 180 kg of sand, 22.5 kg of film-forming aids, and 460 kg of acrylic emulsion.
[0015]
[0016] When preparing, first put the above water into the mixing tank, slowly add hydroxyethyl cellulose under low-speed stirring, stir for 20 minutes, then slowly add dispersant, defoamer, bactericide, antifreeze, regulator, and stir for 15 minutes at low speed. Minutes, then slowly put calcium carbonate, titanium dioxide, and quartz sand into the mixing tank, stir at high speed for 30 minutes, then put in film-forming aids and acrylic acid emulsion, stir at low speed for 15 minutes, and take out the materials to obtain the new anti-yellowing interface agent.
Embodiment 2
[0018] Take 150 kg of water, 4 kg of hydroxyethyl cellulose, 3 kg of dispersant, 2 kg of defoamer, 1 kg of bactericide, 22 kg of antifreeze, 0.5 kg of regulator, 90 kg of calcium carbonate, 60 kg of titanium dioxide, quartz 160 kg of sand, 25 kg of film-forming aids, and 480 kg of acrylic emulsion.
[0019] When preparing, first put the above water into the mixing tank, slowly add hydroxyethyl cellulose under low-speed stirring, stir for 20 minutes, then slowly add dispersant, defoamer, bactericide, antifreeze, regulator, and stir for 15 minutes at low speed. Minutes, then slowly put calcium carbonate, titanium dioxide, and quartz sand into the mixing tank, stir at high speed for 30 minutes, then put in film-forming aids and acrylic acid emulsion, stir at low speed for 15 minutes, and take out the materials to obtain the new anti-yellowing interface agent.
Embodiment 3
[0021] Take 170 kg of water, 4.6 kg of hydroxyethyl cellulose, 4.5 kg of dispersant, 2.5 kg of defoamer, 2 kg of bactericide, 25 kg of antifreeze, 0.8 kg of regulator, 70 kg of calcium carbonate, 45 kg of titanium dioxide, quartz 170 kg of sand, 27 kg of film-forming aids, and 470 kg of acrylic emulsion.
[0022] When preparing, first put the above water into the mixing tank, slowly add hydroxyethyl cellulose under low-speed stirring, stir for 20 minutes, then slowly add dispersant, defoamer, bactericide, antifreeze, regulator, and stir for 15 minutes at low speed. Minutes, then slowly put calcium carbonate, titanium dioxide, and quartz sand into the mixing tank, stir at high speed for 30 minutes, then put in film-forming aids and acrylic acid emulsion, stir at low speed for 15 minutes, and take out the materials to obtain the new anti-yellowing interface agent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com