A production method and technology of mineral dressing agent, applied in the field of environment-friendly gold mineral dressing agent, can solve problems such as skin, oral cavity trauma, long leaching time, etc., and achieve the effect of low production cost and shortened production and processing time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A kind of environment-friendly type gold beneficiation agent and production method thereof, the steps of the present invention are:
[0019] 1) Preparation of mineral dressing agent: mix yellow blood salt and urea according to the weight ratio of 1:1, put it in the boiler, add glass sodium sulfate during the slow heating process, heat to molten state, continue to add glass sodium sulfate to melt The pH value of the product is controlled at 9.5, and the melting temperature is maintained for 30 minutes, then poured out and cooled to normal temperature to obtain the mineral dressing agent;
[0020] 2) Preparation before recovery: recover precious metals as gold; take 1 ton of gold mineral powder, the mineral powder contains 4 grams of gold per ton, use 250 grams of mineral dressing agent, add 30 kg of lime per ton of mineral powder and mix According to the dosage of mineral dressing agent, 1000 kg of water is added to dissolve it, and the ore powder after adding lime is so...
Embodiment 2
[0023] A kind of environment-friendly type gold beneficiation agent and production method thereof, the steps of the present invention are:
[0024] 1) Preparation of mineral dressing agent: mix yellow blood salt and urea according to the weight ratio of 1:4, put it in the boiler, add glass sodium sulfate during the slow heating process, heat to molten state, continue to add glass sodium sulfate to melt The pH value of the product is controlled at 10, the melting temperature is maintained for 40 minutes, and then poured out and cooled to normal temperature to obtain the mineral dressing agent;
[0025] 2) Preparation before recovery: recover precious metals as gold; take 1 ton of gold mineral powder, the mineral powder contains 4 grams of gold per ton, use 300 grams of mineral dressing agent, add 40 kg of lime per ton of mineral powder and mix According to the dosage of mineral dressing agent, add 1500 kg of water to dissolve, soak or heap the ore powder after adding lime accor...
Embodiment 3
[0027] A kind of environment-friendly type gold beneficiation agent and production method thereof, the steps of the present invention are:
[0028] 1) Preparation of mineral dressing agent: mix yellow blood salt and urea according to the weight ratio of 1:8, put it in the boiler, add glass sodium sulfate during the slow heating process, after heating to molten state, continue to add glass sodium sulfate to melt The pH value of the product is controlled at 10.5, and the melting temperature is maintained for 35 minutes, then poured out and cooled to normal temperature to obtain the mineral dressing agent;
[0029] 2) Preparation before recovery: recover precious metals as gold; take 1 ton of gold mineral powder, the mineral powder contains 4 grams of gold per ton, use 275 grams of mineral dressing agent, add 35 kg of lime per ton of mineral powder and mix According to the dosage of mineral dressing agent, add 1250 kg of water to dissolve, soak or heap the ore powder after adding...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com