Dyeing method for multilevel-color jean yarns
A multi-layer, yarn technology, applied in dyeing, textiles and papermaking, etc., can solve the problems of low energy consumption in room temperature dyeing, reduce production costs, shorten the process flow, etc., achieve simple and easy to control washing, reduce production costs, shorten The effect of the process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0040] Example 1: A continuous pad dyeing dyeing method of dope brilliant blue on 16s denim yarn. Follow the steps below to implement:
[0041] (1) Refining treatment of yarn
[0042] Caustic soda: 3g / L
[0043] Penetrant: 4g / L
[0044] Temperature: 60°C
[0045] (2) Cationic modification of yarn
[0046] Cationic modifier: 14g / L
[0047] Caustic soda: 6g / L
[0048] Temperature: 50°C
[0049] (3) Configuration of paint dye solution
[0050] Paint Brilliant Blue: 20g / L
[0051] Softener: 5g / L
[0052] Penetrant: 4g / L
[0053] Cross-linking agent: 4g / L
[0054] Binder: 15g / L
[0055] (4) Configuration of indigo dyeing solution
[0056] Indigo: 1.8g / L
[0057] Hydrosulfite: 0.7g / L
[0058] Caustic soda: 3.2g / L
[0059] (5) Production process:
[0060] Refining→washing→cation modification treatment→pre-baking→1 coat→4 coats of indigo→washing→sizing→drying
[0061] (6) Process parameters:
[0062] Surplus rate: 70%
[0063] Drying temperature: 120°C
[0064]Ind...
Embodiment 2
[0067] Example 2: A continuous pad dyeing method of pretreated Tu Feihong on 16s denim yarn. Follow the steps below to implement:
[0068] (1) Refining treatment of yarn
[0069] Caustic soda: 3g / L
[0070] Penetrant: 4g / L
[0071] Temperature: 60°C
[0072] (2) Preparation of cationic modification solution for yarn
[0073] Cationic modifier: 14g / L
[0074] Caustic soda: 6g / L
[0075] Temperature: 50°C
[0076] (3) Preparation of paint dye solution
[0077] Pigment Feihong: 15g / L
[0078] Softener: 5g / L
[0079] Penetrant: 4g / L
[0080] Cross-linking agent: 4g / L
[0081] Binder: 15g / L
[0082] (4) Preparation of indigo dyeing solution
[0083] Indigo: 2.55g / L
[0084] Hydrosulfite: 0.75g / L
[0085] Caustic soda: 3.0g / L
[0086] (5) Production process:
[0087] Refining→washing→cation modification treatment→pre-baking→1 coat→4 coats of indigo→washing→sizing→drying
[0088] (6) Process parameters:
[0089] Surplus rate: 70%
[0090] Drying temperature: 120°C...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com