Embodiment 1
[0016] Negative ion air purifier, containing Na + The concentration is 6.8mg / L, K + The concentration is 5.0mg / L, Mg 2+ The concentration is ≤0.01mg / L, Ca 2+ The concentration is 0.05mg / L, Si 2+ The concentration is 0.7mg / L.
[0017] Its specific preparation method is as follows:
[0018] Weigh wollastonite according to the concentration of silicon ions and crush it, then concentrate seawater 5 times to become concentrated seawater mother liquor; weigh potassium halite and sodium bicarbonate respectively according to the concentration of potassium ions and sodium ions, add potassium halite to seawater to concentrate After being uniformly dissolved in the mother liquor, wollastonite and sodium bicarbonate are added to the concentrated seawater mother liquor and reacted at room temperature for 5 hours to prepare an anion air purifier.
Embodiment 2
[0020] Negative ion air purifier, containing Na + The concentration is 6.5mg / L, K + The concentration is 4.7mg / L, Mg 2+ The concentration is ≤0.01mg / L, Ca 2+ The concentration is 0.04mg / L, Si 2+ The concentration is 0.68mg / L.
[0021] Its specific preparation method is as follows:
[0022] Weigh wollastonite according to the concentration of silicon ions and crush it, then concentrate seawater 3 times to become concentrated seawater mother liquor; weigh potassium halite and sodium bicarbonate respectively according to the concentration of potassium ions and sodium ions, add potassium halite to seawater to concentrate After being uniformly dissolved in the mother liquor, wollastonite and sodium bicarbonate are added to the concentrated seawater mother liquor and reacted at room temperature for 5 hours to prepare an anion air purifier.
Embodiment 3
[0024] Negative ion air purifier, containing Na + The concentration is 6.3mg / L, K + The concentration is 4.5mg / L, Mg 2+ The concentration is ≤0.01mg / L, Ca 2+ The concentration is 0.03mg / L, Si 2+ The concentration is 0.65mg / L.
[0025] Its specific preparation method is as follows:
[0026] Weigh wollastonite according to the silicon ion concentration and pulverize it, then concentrate the seawater by 1 time to become the concentrated seawater mother liquor; weigh potassium halite and sodium bicarbonate respectively according to the concentration of potassium ions and sodium ions, add potassium halite to seawater to concentrate After being uniformly dissolved in the mother liquor, wollastonite and sodium bicarbonate are added to the concentrated seawater mother liquor and reacted at room temperature for 5 hours to prepare an anion air purifier.