Printing method of polar fleece bended fabric
A technology of blended fabrics and printing methods, which is applied in the field of printing of polar fleece blended fabrics, can solve problems such as difficult product quality to meet market requirements, and achieve the effects of improving operation production efficiency, improving product quality, and high rubbing fastness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A printing method for polar fleece blended fabrics, comprising the following steps:
[0018] (1) Pre-treatment: put the fabric to be printed into a washing machine in bags for one wash, add 4g / L anionic surfactant sodium alkyl sulfate and 1g / L dip dyeing refining agent, the temperature is 45°C, and the liquor ratio is 1 :16, soaked for 15 minutes and washed with water for 20 minutes; then add 3g / L hydrogen peroxide, soak for 15 minutes and then wash with water for the second time, the temperature is 35°C, the bath ratio is 1:16, and the washed time is 20 minutes; finally add 5g / L of silicone softener soaked for 25 minutes and then dehydrated to 70% dry;
[0019] (2) Printing: The pre-treated fabric is processed by jet printing, and the printing dye is prepared according to the following formula by weight: 15% neutral dye, 5% sodium alginate, ultraviolet absorption 0.5% dispersant, 2% sodium acetate, 0.5% dispersant, and the rest of water; after all the raw materials a...
Embodiment 2
[0023] A printing method for polar fleece blended fabrics, comprising the following steps:
[0024] (1) Pre-treatment: put the fabric to be printed into a washing machine in bags for one wash, add 8g / L anionic surfactant sodium alkyl sulfate and 3g / L dip dyeing refining agent, the temperature is 55°C, and the liquor ratio is 1 :20, soaked for 15 minutes and washed with water for 30 minutes; then added 7g / L hydrogen peroxide, soaked for 15 minutes and then washed with water for the second time, the temperature was 45°C, the bath ratio was 1:20, and the washed time was 30 minutes; finally added 15g / L of silicone softener soaked for 25 minutes and then dehydrated to 80% dry;
[0025] (2) Printing: The pre-treated fabric is processed by jet printing, and the printing dye is prepared according to the following formula by weight: 45% neutral dye, 15% sodium alginate, ultraviolet absorption 3.0% sodium acetate, 6% sodium acetate, 2.0% dispersant, and the rest of water; after all th...
Embodiment 3
[0029] A printing method for polar fleece blended fabrics, comprising the following steps:
[0030] (1) Pre-treatment: put the fabric to be printed into a washing machine in bags for one wash, add 6g / L anionic surfactant sodium alkyl sulfate and 2g / L dip dyeing refining agent, the temperature is 50°C, and the liquor ratio is 1 :18, soaked for 15 minutes and then washed with water for 25 minutes; then added 5g / L of hydrogen peroxide, soaked for 15 minutes and then washed with water for the second time, the temperature was 40°C, the bath ratio was 1:18, and the washed time was 25 minutes; finally added 10g / L of silicone softener soaked for 25 minutes and then dehydrated to 70% dry;
[0031] (2) Printing: The pre-treated fabric is processed by jet printing, and the printing dye is prepared according to the following formula by weight: 25% neutral dye, 10% sodium alginate, ultraviolet absorption 1.5% dispersant, 4% sodium acetate, 1.3% dispersant, and the rest of water; after pr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com