Preparation method of hot melt pressure-sensitive adhesive material
A hot-melt adhesive and glue technology, applied in the field of daily necessities, can solve the problems of low service life, weak initial viscosity, insufficient grip, etc., and achieve the effect of improving environmental protection.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0022] A kind of preparation method of hot-melt adhesive type self-adhesive material described in the embodiment of the present invention, the preparation method of this self-adhesive material comprises the following steps:
[0023] ① Preparation of solvent-free composite backing paper: coating the backing paper with a solvent-free solution, and the process is carried out on a coating device. The components of the solvent-free solution and the parts by weight of each component are solvent-free silicone 110, Platinum complex 3 and methyl hydrogen-containing silicone oil 4.5; the coating speed is 110 m / min, and the amount of solvent-free solution coated is 1.1 to 1.2 g / m2; the coating device is connected to a 30m long oven, and the coating The coating device transports the coated backing paper to an oven for drying, and the drying temperature is 140° C. to obtain the solvent-free composite backing paper; ② Raw materials for glue: the parts by weight of various components in the r...
Embodiment
[0027] ① Preparation of solvent-free composite backing paper: coating the backing paper with a solvent-free solution, and the process is carried out on a coating device. The components of the solvent-free solution and the parts by weight of each component are solvent-free silicone 110, Platinum complex 3 and methyl hydrogen-containing silicone oil 4.5; the coating speed is 110 m / min, and the amount of solvent-free solution coated is 1.1 to 1.2 g / m2; the coating device is connected to a 30m long oven, and the coating The coating device transports the coated backing paper to an oven for drying, and the drying temperature is 140°C to obtain the solvent-free composite backing paper;
[0028] ②Preparation of glue: When the temperature of the reaction boiler is increased to 200°C, add 10kg of white ring oil, stir for 10 minutes, add 25kg of thermoplastic rubber and 25kg of thermoplastic elastomer, continue stirring to melt the rubber, and then add 20kg of terpene resin, Put 19kg of ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com