Keratin hair conditioner and preparation method thereof
A hair conditioner and keratin technology, applied in the field of daily chemicals, can solve problems such as difficult combing, easy dirtying, lack of luster, etc., and achieve the effects of uniform spreading, improved softness, and accelerated penetration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Take the following raw materials by weight percentage respectively: 81.6% water, 3.0% propylene glycol, 5.0% cetearyl alcohol, 1.2% behenyl trimethyl ammonium chloride, 1.2% glyceryl stearate, 1.2% cetyl trimethyl ammonium chloride, 0.2% methylparaben, 0.1% propylparaben, 1.0% cyclopentasiloxane, 0.5% C 12-15 Parabens, 1.0% Dimethicone, 0.5% Dimethicone, 1.5% Olive Oil, 0.5% Sodium Pyrrolidone Carboxylate, 0.5% Hydrolyzed Keratin, 0.5% Provitamin B5, 0.1% 2- Methyl-4-isothiazolin-3-one and 0.4% fragrance.
[0024] Add the above-mentioned raw materials into the vacuum emulsification pot according to the following steps to prepare the keratin conditioner:
[0025] a. Add component A composed of water and propylene glycol into the water phase pot and raise the temperature to 85°C, then pump it into the emulsification pot;
[0026] b. A composition consisting of cetearyl alcohol, behenyltrimethylammonium chloride, glyceryl stearate, cetyltrimethylammonium chloride, methyl...
Embodiment 2
[0030] Take the following raw materials by weight percentage respectively: 70.5% water, 5.0% propylene glycol, 7.0% cetearyl alcohol, 2.0% behenyl trimethyl ammonium chloride, 2.0% glyceryl stearate, 2.0% cetyl trimethyl ammonium chloride, 0.2% methylparaben, 0.1% propylparaben, 2.0% cyclopentasiloxane, 1.0% C 12-15 Parabens, 1.5% Dimethicone, 1.0% Dimethicone, 2.0% Olive Oil, 1.0% Sodium Pyrrolidone Carboxylate, 1.0% Hydrolyzed Keratin, 0.8% Provitamin B5, 0.1% 2- Methyl-4-isothiazolin-3-one and 0.8% fragrance.
[0031] Add the above-mentioned raw materials into the vacuum emulsification pot according to the following steps to prepare the keratin conditioner:
[0032] a. Add component A composed of water and propylene glycol into the water phase pot and raise the temperature to 85°C, then pump it into the emulsification pot;
[0033] b. A composition consisting of cetearyl alcohol, behenyltrimethylammonium chloride, glyceryl stearate, cetyltrimethylammonium chloride, methyl...
Embodiment 3
[0037] Take the following raw materials by weight percentage respectively: 75.2% water, 4.0% propylene glycol, 6.0% cetearyl alcohol, 1.5% behenyl trimethyl ammonium chloride, 1.5% glyceryl stearate, 2.0% cetyl trimethyl ammonium chloride, 0.2% methylparaben, 0.1% propylparaben, 2.0% cyclopentasiloxane, 0.8% C 12-15 Parabens, 1.2% Dimethicone, 0.8% Diaminosiloxane, 1.8% Olive Oil, 0.8% Sodium Pyrrolidone Carboxylate, 0.6% Hydrolyzed Keratin, 0.6% Provitamin B5, 0.1% 2- Methyl-4-isothiazolin-3-one and 0.8% fragrance.
[0038] Add the above-mentioned raw materials into the vacuum emulsification pot according to the following steps to prepare the keratin conditioner:
[0039] a. Add component A composed of water and propylene glycol into the water phase pot and raise the temperature to 85°C, then pump it into the emulsification pot;
[0040] b. A composition consisting of cetearyl alcohol, behenyltrimethylammonium chloride, glyceryl stearate, cetyltrimethylammonium chloride, me...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com