[0015] A kind of multi-color pattern paint, its raw material ratio by weight is as follows: polyvinyl chloride 100 parts; Methanol 25 parts; Lead chromate 30 parts; Polyvinyl butyral 10 parts; Calcium carbonate 35 parts; Ethylene glycol 10 parts 80 parts of deionized water; 15 parts of nitrile rubber; 10 parts of iron oxide green; 5 parts of isobutyl isobutyrate; 40 parts of toluene; 15 parts of isobutyl acetate; 4 parts of dibutyl phthalate; 25 parts of isopropanol; 30 parts of vinylidene chloride; 25 parts of methyl ethyl ketone.
[0016] Add polyvinyl chloride, lead chromate, polyvinyl butyral, calcium carbonate and ethylene glycol into deionized water, heat to 40°C and stir for 3 hours, add nitrile rubber, isobutyl isobutyrate, toluene, isoacetic acid Butyl ester, vinylidene chloride and dibutyl phthalate, heat up to 50°C and use a ball mill to mill for 10 minutes, add methanol and the remaining raw materials, heat up to 60°C and stir for 10 hours to obtain the finished pr...
Embodiment 2
[0019] A kind of multi-color pattern coating, its raw material ratio by weight is as follows: polyvinyl chloride 100 parts; Methanol 35 parts; Lead chromate 40 parts; Polyvinyl butyral 20 parts; Calcium carbonate 45 parts; Ethylene glycol 20 parts 90 parts of deionized water; 35 parts of nitrile rubber; 20 parts of iron oxide yellow; 15 parts of isobutyl isobutyrate; 50 parts of toluene; 25 parts of isobutyl acetate; 10 parts of dibutyl phthalate; 45 parts of isopropanol; 40 parts of vinylidene chloride; 35 parts of methyl ethyl ketone.
[0020] Add polyvinyl chloride, lead chromate, polyvinyl butyral, calcium carbonate and ethylene glycol into deionized water, heat to 40°C and stir for 3 hours, add nitrile rubber, isobutyl isobutyrate, toluene, isoacetic acid Butyl ester, vinylidene chloride and dibutyl phthalate, heat up to 50°C and use a ball mill to mill for 10 minutes, add methanol and the remaining raw materials, heat up to 60°C and stir for 10 hours to obtain the finish...
Embodiment 3
[0023] A kind of multi-color pattern paint, its raw material ratio by weight is as follows: 100 parts of polyvinyl chloride; 30 parts of methanol; 35 parts of lead chromate; 15 parts of polyvinyl butyral; 40 parts of calcium carbonate; 85 parts of deionized water; 25 parts of nitrile rubber; 15 parts of iron oxide red; 10 parts of isobutyl isobutyrate; 45 parts of toluene; 20 parts of isobutyl acetate; 7 parts of dibutyl phthalate; 35 parts of isopropanol; 35 parts of vinylidene chloride; 30 parts of methyl ethyl ketone.
[0024] Add polyvinyl chloride, lead chromate, polyvinyl butyral, calcium carbonate and ethylene glycol into deionized water, heat to 40°C and stir for 3 hours, add nitrile rubber, isobutyl isobutyrate, toluene, isoacetic acid Butyl ester, vinylidene chloride and dibutyl phthalate, heat up to 50°C and use a ball mill to mill for 10 minutes, add methanol and the remaining raw materials, heat up to 60°C and stir for 10 hours to obtain the finished product.
[...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com