A crack and gas prevention technology, applied in the field of oil drilling, can solve the problems of no compressibility of the plugging layer, gas intrusion overflow, unable to obtain compressibility and lead to sealing and plugging, etc., so as to reduce permeability and prevent gas intrusion. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] The preparation method of the anti-gas intrusion agent for sealing cracks while drilling:
[0047] 1) Weigh 15.2 parts of polyethylene glycol and add it to 260 parts by mass of water, let it stand at room temperature for 40 minutes, then stir and mix evenly at a constant temperature of 35°C;
[0048] 2) Weigh 25.5 parts by mass of maleic anhydride and 25.5 parts of trimethylolpropane diallyl ether, add them to the above solution, stir and mix evenly;
[0049] 3) Heat the above solution to 50°C, and adjust the pH value of the solution to 9 with a pH regulator;
[0050] 4) Add an initiator, stir and react with the above mixed solution at 80°C for 100 minutes, and react to obtain a viscous polymer;
[0051] 5) Dry the viscous polymer at 104°C, grind and pulverize it through a 20-mesh sieve to obtain polymer particles;
[0052] 6) Sequentially weigh 0.5 parts by mass of bentonite, 35 parts of superfine calcium carbonate powder, and 5.0 parts of cotton fiber, add them to t...
Embodiment 2
[0055] The preparation method of the anti-gas intrusion agent for sealing cracks while drilling,
[0056] 1) Weigh 10.0 parts of polyethylene glycol and add it to 180 parts by mass of water, let it stand at room temperature for 30 minutes, then stir and mix evenly at a constant temperature of 30°C;
[0057] 2) Weigh 14.0 parts by mass of maleic anhydride and 14.5 parts of trimethylolpropane diallyl ether, add them to the above solution, stir and mix evenly;
[0058] 3) Heat the above solution to 40°C, and adjust the pH value of the solution to 7 with a pH regulator;
[0059] 4) Add an initiator, stir and react with the above mixed solution at 60°C for 60 minutes, and react to obtain a viscous polymer;
[0060] 5) Dry the viscous polymer at 90°C, grind and pulverize it through a 20-mesh sieve to obtain polymer particles;
[0061] 6) Sequentially weigh 0.2 parts of bentonite, 30 parts of superfine calcium carbonate powder, and 3.0 parts of cotton fiber into the polymer particl...
Embodiment 3
[0064] The preparation method of the anti-gas intrusion agent for sealing cracks while drilling,
[0065] 1) Weigh 12.2 parts of polyethylene glycol and add 200 parts by mass of water, let it stand at room temperature for 35 minutes, then stir and mix evenly at a constant temperature of 32°C;
[0066] 2) Weigh 20.5 parts by mass of maleic anhydride and 20.5 parts of trimethylolpropane diallyl ether, add them to the above solution, stir and mix evenly;
[0067] 3) Heat the above solution to 45°C, and adjust the pH value of the solution to 8 with a pH regulator;
[0068] 4) Add an initiator, stir and react with the above mixed solution at 70°C for 80 minutes, and react to obtain a viscous polymer;
[0069] 5) Dry the viscous polymer at 100°C, grind and pulverize it through a 20-mesh sieve to obtain polymer particles;
[0070] 6) Sequentially weigh 0.4 parts by mass of bentonite, 32 parts of superfine calcium carbonate powder, and 4.0 parts of cotton fiber, add them to the poly...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com