Slagging agent produced by high-purity vanadium-aluminium alloy and production method
The technology of a vanadium-aluminum alloy and a production method, which is applied in the field of vanadium alloy production, can solve the problems of increasing the production cost and high price of the vanadium-aluminum alloy, and achieve the effects of low production raw materials and cost, low product cost, and reduced production cost.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Embodiment 1: The production method of this high-purity vanadium-aluminum alloy adopts the following slagging agent and production process.
[0033] Mix 1667kg of calcium metavanadate with 500kg of vanadium pentoxide (mass ratio 1:0.3) and put them into the reaction furnace (device) with 1183kg of aluminum particles (powder). After being separated from vanadium-aluminum alloy, 85 vanadium-aluminum alloy is obtained after grinding, crushing and sorting. The composition (weight) of the obtained vanadium aluminum alloy is: V 86.32%, Al 12.98%, N 0.0004%, O 0.05%, C 0.10%, S 0.004%, Cr 0.071%, Fe 0.251%, Mg 0.012%, Mn 0.019% , P 0.03%, Si 0.097%.
Embodiment 2
[0034]Embodiment 2: The production method of this high-purity vanadium-aluminum alloy adopts the following slagging agent and production process.
[0035] Mix 590kg of calcium pyrovanadate with 1500kg of vanadium pentoxide (mass ratio 1:2.55) and put them into the reaction furnace (device) with 1243kg of aluminum particles (powder). After being separated from vanadium-aluminum alloy, 85 vanadium-aluminum alloy is obtained after grinding, crushing and sorting. The composition of the obtained vanadium aluminum alloy is: V 89.23%, Al 10.21%, N 0.0005%, O 0.045%, C 0.009%, S 0.005%, Cr 0.070%, Fe 0.241%, Mg 0.010%, Mn 0.020%, P 0.025 %, Si 0.095%.
Embodiment 3
[0036] Embodiment 3: The production method of high-purity vanadium-aluminum alloy adopts the following slagging agent and production process.
[0037] Mix 460kg of calcium orthovanadate with 1633kg of vanadium pentoxide (mass ratio 1:3.5) and put them into the reaction furnace (device) with 1248kg of aluminum particles (powder). After being separated from vanadium-aluminum alloy, 85 vanadium-aluminum alloy is obtained after grinding, crushing and sorting. The composition of the obtained vanadium aluminum alloy is: V 89.02%, Al 10.47%, N 0.0005%, O 0.035%, C 0.095%, S 0.005%, Cr 0.069%, Fe 0.228%, Mg 0.012%, Mn 0.017%, P 0.028 %, Si 0.087%.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com