Rubber explosive for explosion hardening
A technology of rubber explosives and explosive hardening, applied in explosives, explosives processing equipment, offensive equipment, etc., can solve the problems of poor low temperature resistance, toxic manufacturing process, and difficult molding, etc., to achieve less human injury, uniform components, and explosive performance Improved effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0013] A rubber explosive for explosive hardening, which is prepared through the following steps: (a) Add 120# solvent gasoline into the container, put the natural rubber in the gasoline, and let it stand for 24h~30h (optional 24h, 25h, 26h, 27h, 28h, 29h, 30h) to make it swell; the mass ratio of natural rubber to 120# solvent gasoline is 1:2.5~2.8 (optional 1:2.5, 1:2.6, 1:2.7, 1:2.8); ( b) Dissolve the binder in another 120# solvent gasoline. The binder is composed of polyisobutylene with a molecular weight of 3000 and polyisobutylene with a molecular weight of 200,000. The mass ratio of isobutylene and 120# solvent gasoline is 4:1:10~13 (4:1:10, 4:1:11, 4:1:12, 4:1:13 can be selected); (c) Preparation Additive mixing system: mix the natural rubber solution prepared in steps (a) and (b) with the binder solution, then add plasticizer, rubber accelerator, oxidant and mix evenly. The plasticizer is Sebi Dioctyl acid, the rubber accelerator is tetramethylthiuram disulfide, and ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com