Coking additive for improving coke performance and coking method
An additive and performance technology, applied in the new energy-saving field, can solve the problems of unsatisfactory reactivity and strength of coke and coke, and achieve the effects of safe and convenient mixing and transportation, improved strength and obvious effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The additive is composed of a surface activation catalyst, a dissolution aid, a penetration aid and an oily solvent; the surface activation catalyst is 1 weight part of SiC powder, 3 weight parts of sodium naphthenate; the dissolution aid is α-hydroxypropionamide 1 parts by weight, 2 parts by weight of acetylthiophene and 1.25 parts by weight of p-toluenesulfonic acid; the penetration aid is 1 part by weight of polyoxyethylene polyoxypropylene monobutyl ether, polyoxyethylene sorbitan tristearic acid 3 parts by weight of ester, 2 parts by weight of chlorophenyl silicone oil and 1.7 parts by weight of triethanolamine molybdenum; the oily solvent is 1 part by weight of coal tar, 2 parts by weight of asphalt and 2 parts by weight of residual oil; agent, penetration aid and oily solvent in the weight ratio of the additive is 1:1.8:1.6:2;
[0016] During coking, the above-mentioned coking additives are added to the coal, wherein the addition amount of the additives in the co...
Embodiment 2
[0019] The additive is composed of a surface activation catalyst, a dissolution aid, a penetration aid and an oily solvent; the surface activation catalyst is 2 parts by weight of SiC powder, 6 parts by weight of sodium naphthenate; the dissolution aid is α-hydroxypropionamide 2 parts by weight, 4 parts by weight of acetylthiophene and 2.5 parts by weight of p-toluenesulfonic acid; the penetration aid is 2 parts by weight of polyoxyethylene polyoxypropylene monobutyl ether, polyoxyethylene sorbitan tristearic acid 6 parts by weight of ester, 4 parts by weight of chlorophenyl silicone oil and 3.4 parts by weight of triethanolamine molybdenum; the oily solvent is 2 parts by weight of coal tar, 4 parts by weight of asphalt and 4 parts by weight of residual oil; agent, penetration aid and oily solvent in the weight ratio of the additive is 1:1.8:1.6:2;
[0020] During coking, the above-mentioned coking additive is added to the coal, wherein the addition amount of the additive in t...
PUM
Property | Measurement | Unit |
---|---|---|
strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com