Anti-bacterial, anti-static and anti-corrosive rubber floor
A rubber floor, anti-corrosion technology, used in anti-corrosion coatings, coatings, etc., can solve the problems of only anti-static, only anti-bacterial, no comprehensive anti-bacterial, anti-static and anti-corrosion floors, etc., to enhance hydrophobicity. Sexuality, prolonged use, strength-enhancing effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] An antibacterial, antistatic and anticorrosion rubber floor of the present invention consists of the following components by weight:
[0019] 20 parts of chloroprene rubber, 38 parts of nitrile rubber, 30 parts of EPDM rubber, 2 parts of magnesium oxide, 0.8 parts of stearic acid, 25 parts of semi-reinforced furnace black, 7 parts of zinc oxide, thiuram accelerator 0.4 parts, 5 parts of 2,2,4-trimethyl-1,2-dihydroquinoline polymer, 1.5 parts of isothiazolinone, 0.8 parts of calcium hypochlorite, 3.2 parts of conductive fiber.
Embodiment 2
[0021] The only difference between this embodiment and embodiment 1 is that the top layer is rubber, and the rubber composition is: in parts by weight,
[0022] 30 parts of chloroprene rubber, 33 parts of nitrile rubber, 25 parts of EPDM rubber, 3 parts of magnesium oxide, 1.3 parts of stearic acid, 17 parts of semi-reinforced furnace black, 4 parts of zinc oxide, thiuram accelerator 0.7 parts, 2,2,4-trimethyl-1,2-dihydroquinoline polymer 7 parts, isothiazolinone 1.8 parts, calcium hypochlorite 0.5 parts, conductive fiber 4.5 parts.
Embodiment 3
[0024] The only difference between this embodiment and embodiment 1 is that the top layer is rubber, and the rubber composition is: in parts by weight,
[0025] 25 parts of chloroprene rubber, 37 parts of nitrile rubber, 28 parts of EPDM rubber, 4 parts of magnesium oxide, 1 part of stearic acid, 23 parts of semi-reinforced furnace black, 6 parts of zinc oxide, thiuram accelerator 0.6 parts, 2,2,4-trimethyl-1,2-dihydroquinoline polymer 6 parts, isothiazolinone 1.6 parts, calcium hypochlorite 0.6 parts, conductive fiber 4.
[0026] The rubber floor is coated with an anti-corrosion coating, and the raw materials of the anti-corrosion coating include by weight: 40 parts of acrylic resin, 48 parts of composite polybenzoxazine material, 17 parts of aldehyde and ketone resin KR-80F, and 0.5 parts of paraffin , 0.1 parts of zirconium chloride, 5 parts of lignin fiber, 1.2 parts of aluminum-zirconium coupling agent TL-4, 2.5 parts of curing agent, 0.1 part of dispersing agent, 1.3 par...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com