Macromolecular framework material capable of absorbing formaldehyde in air and preparation method of macromolecular framework material
A polymer skeleton and skeleton technology, applied in separation methods, chemical instruments and methods, and other chemical processes, can solve the problems of imperfect degradation methods, human injury, and high costs, and achieve ideal results, cost reduction, and problem simplification. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0020] The present invention will be described in further detail below in conjunction with the embodiments.
[0021] Material preparation: First prepare a water-soluble copolymer, mix N,N-dimethylacrylamide and glycidyl methacrylate in a molar ratio of 12:1 to 15:1, add an equal volume of methanol as a solvent, and initiate with AIBN and polymerize for 10-12 hours in the temperature range of 60-65°C. After the polymerization is sufficient, the methanol is removed in vacuo to obtain a solid polymer, which is then prepared into a 2-3wt.% aqueous solution, and the prepared aqueous solution is mixed with an equal volume of 0.5-0.6wt.% .% polyethyleneimine (number average molecular weight is 600-700) acetic acid aqueous solution (keeping the pH value of the solution in the range of 4-5) is mixed and stirred, and a commercially available melamine sponge (melamine and formaldehyde cross-linking reaction is prepared The foam material, which is now commercialized), is immersed in the m...
PUM
| Property | Measurement | Unit |
|---|---|---|
| size | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
Abstract
Description