A fine-scale, low-grade technology, applied in the field of low-grade fine-scale graphite mineral processing and purification process, can solve the problems of unreasonable middling treatment, low regrinding efficiency, and long regrinding process, so as to reduce mineral processing costs and improve concentrate The effect of fixed carbon content and low foam viscosity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] A low-grade fine flake graphite ore dressing and purification process, the process flow chart is shown in figure 1 , including the following steps:
[0032] A. Put the low-grade fine flake graphite raw ore with fixed carbon content of 8.93% into the jaw crusher for coarse crushing. The particle size of the coarsely crushed product is 10-15mm, and then put the coarsely crushed product into the roller crusher for fine crushing to -2mm. Use conical ball mill for coarse grinding, the grinding concentration is 65%, the grinding fineness is -0.074mm, and the content is 88.95%; add inhibitor quicklime and regulator water glass to the obtained ground low-grade fine flake graphite ore , Collector kerosene and foaming agent 2-octanol are fully stirred and roughed, the roughing concentration is 25%, the roughing time is 6.5min, and the rough concentrate and tailings a are obtained; the roughing agent formula is per ton Add 1500g of quicklime, 800g of water glass, 360g of kerosen...
Embodiment 2
[0043] A low-grade fine flake graphite ore dressing purification process, it comprises the following steps:
[0044] A. Put the low-grade fine flake graphite raw ore with fixed carbon content of 10.55% into the jaw crusher for coarse crushing, the coarse crushed product has a particle size of 10-15mm, and then put the coarse crushed product into the roller crusher for fine crushing to -2mm, Use conical ball mill for coarse grinding, the grinding concentration is 65%, the grinding fineness is -0.074mm, and the content is 87.89%; add inhibitor quicklime and regulator water glass to the obtained ground low-grade fine flake graphite raw ore , Collector kerosene and foaming agent 2-octanol are fully stirred and roughed, the roughing concentration is 25%, the roughing time is 7min, and the rough concentrate and tailings a are obtained; the formula of the roughing agent is low Add 1500g of quicklime, 1000g of water glass, 400g of kerosene and 100g of secondary octanol to the raw ore ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com