A flotation agent and coal preparation technology, applied in flotation, solid separation, etc., can solve the problems of poor flotation performance, large amount of agent used, cumbersome operation procedures, etc., to overcome the poor stability of agent and the reduction of agent dosage , The effect of simplifying the process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] The composite coal preparation flotation agent is composed of 50% of light diesel oil, 0.5% of sodium lauryl sulfate, 0.4% of alkyl glucoside, 3% of alkylphenol polyoxyethylene ether and 46% of water in mass percentage. Sodium lauryl sulfate, alkyl glucoside, and alkylphenol polyoxyethylene ether were respectively configured into aqueous solutions with a mass fraction of 5%, 10%, and 20%, and then 25mL of light diesel oil was added to the reaction vessel, and magnetically Add 5mL sodium lauryl sulfate, 2.5mL alkyl glucoside and 7.5mL alkylphenol polyoxyethylene ether under the condition of stirring. After stirring for 5 minutes, use a high-speed cutting emulsifier to emulsify at a working speed of 3000r / min for 10 minutes to obtain Milky white water-soluble compound coal preparation flotation agent.
[0022] The composite coal preparation flotation agent prepared in this example was left to stand naturally at room temperature for 24 hours, and was shaken and shaken in d...
Embodiment 2
[0025] The composite coal preparation flotation agent is composed of 65% of light diesel oil, 0.5% of sodium lauryl sulfate, 0.6% of alkyl glucoside, 4% of alkylphenol polyoxyethylene ether and 40% of water in mass percentage. Sodium lauryl sulfate, alkyl glucoside, and alkylphenol polyoxyethylene ether are respectively configured into aqueous solutions with a mass fraction of 5%, 10% and 20%, and then 32.5mL of light oil is added to the reaction vessel, and at room temperature Under the condition of magnetic stirring, add 5mL sodium lauryl sulfate, 3mL alkyl glucoside and 10mL alkylphenol polyoxyethylene ether, after stirring for 5min, use a high-speed cutting emulsifier to emulsify at a working speed of 2000r / min for 20min to obtain milky white Water-soluble composite coal preparation flotation agent.
[0026] The composite coal preparation flotation agent prepared in this example has good stability at room temperature. The yield of clean coal in flotation experiments is 34....
Embodiment 3
[0028] The composite coal preparation flotation agent is composed of 55% light diesel oil, 0.4% sodium lauryl sulfate, 0.5% alkyl glucoside, 4% alkylphenol polyoxyethylene ether and 40.1% water in mass percentage. Sodium lauryl sulfate, alkyl glucoside, and alkylphenol polyoxyethylene ether were respectively configured into aqueous solutions with a mass fraction of 5%, 10% and 20%, and then 27.5mL of light oil was added to the reaction vessel, and at room temperature Under the condition of magnetic stirring, add 4mL sodium lauryl sulfate, 2.5mL alkyl glycoside and 10mL alkylphenol polyoxyethylene ether, after stirring for 5min, use a high-speed cutting emulsifier to emulsify at a working speed of 2500r / min for 15min to obtain Milky white water-soluble compound coal preparation flotation agent.
[0029] The composite coal preparation flotation agent prepared in this example has good stability at room temperature. The yield of clean coal in flotation experiments is 26.71%, the a...