Embodiment 1
[0012] A leather soft sunscreen finishing agent, which is composed of the following raw materials in parts by weight: 15 parts of fatty alcohol polyoxyethylene ether, 2 parts of sodium xylene sulfonate, 10 parts of alcohol ethoxylate carboxylate, and 1 part of sodium bicarbonate , 4 parts of coupling agent, 7 parts of sophorolipid, 2 parts of surfactant, 5 parts of acetic acid, 1 part of sodium citrate, 1 part of acrylamide, 12 parts of natural saponin, 5 parts of soybean ethyl sulfate ethyl morpholine, 25 parts of base oil, 8 parts of polyoxyethylene sorbitan fatty acid ester.
[0013] The surfactant is one or more of AFCONA3030, AFCONA3031, AFCONA3034, and AFCONA3037.
[0014] The base oil is one or a mixture of wheat germ oil, jojoba oil, avocado oil and nut oil.
[0015] The coupling agent is one or more mixtures of silane coupling agents KH560, KH570, and DL602.
[0016] The method of use is: dilute the leather soft sunscreen finishing agent with water to prepare an aqu...
Embodiment 2
[0018] A leather soft sunscreen finishing agent, which is composed of the following raw materials in parts by weight: 17 parts of fatty alcohol polyoxyethylene ether, 6 parts of sodium xylene sulfonate, 13 parts of alcohol ethoxylate carboxylate, and 2 parts of sodium bicarbonate , 7 parts of coupling agent, 9 parts of sophorolipid, 6 parts of surfactant, 9 parts of acetic acid, 3 parts of sodium citrate, 6 parts of acrylamide, 16 parts of natural saponin, 7 parts of soybean ethyl sulfate ethyl ester morpholine, 29 parts of base oil, 9 parts of polyoxyethylene sorbitan fatty acid ester.
[0019] The surfactant is one or more of AFCONA3030, AFCONA3031, AFCONA3034, and AFCONA3037.
[0020] The base oil is one or a mixture of wheat germ oil, jojoba oil, avocado oil and nut oil.
[0021] The coupling agent is one or more mixtures of silane coupling agents KH560, KH570, and DL602.
[0022] The method of use is: dilute the leather soft sunscreen finishing agent with water to prepa...
Embodiment 3
[0024] A leather soft sunscreen finishing agent, which is composed of the following raw materials in parts by weight: 16 parts of fatty alcohol polyoxyethylene ether, 4 parts of sodium xylene sulfonate, 12 parts of alcohol ethoxylate carboxylate, and 1 part of sodium bicarbonate , 5.5 parts of coupling agent, 8 parts of sophorolipid, 4 parts of surfactant, 5-9 parts of acetic acid, 2 parts of sodium citrate, 4 parts of acrylamide, 14 parts of natural saponin, soybean ethyl sulfate ethyl morpholine 6 parts, base oil 27 parts, polyoxyethylene sorbitan fatty acid ester 9 parts.
[0025] The surfactant is one or more of AFCONA3030, AFCONA3031, AFCONA3034, and AFCONA3037.
[0026] The base oil is one or a mixture of wheat germ oil, jojoba oil, avocado oil and nut oil.
[0027] The coupling agent is one or more mixtures of silane coupling agents KH560, KH570, and DL602.
[0028] The method of use is: dilute the leather soft sunscreen finishing agent with water to prepare an aqueou...