Environment-friendly non-toxic particle floor processed by sawdust and preparation method thereof
An environmentally friendly, wood chip technology, applied in the direction of adhesive types, adhesive additives, polymer adhesive additives, etc., can solve problems such as ineffective effects, save wood resources, improve viscosity, and improve floor strength. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Embodiment 1: A kind of environment-friendly non-toxic shaving floor that utilizes sawdust processing, as attached figure 1 As shown, it includes a skin 1, a core board 2 and a bottom board 3 from top to bottom. The core board 2 includes a particle core board 4 in the middle, and reinforcement bamboo chips 5 are provided on both sides of the particle core board 4. A stress groove 6 is opened at the bottom of the bottom plate 3 . figure 1 In the middle circle is a partial enlarged view of the stress groove, which can be a through groove perpendicular to the length direction of the floor.
Embodiment 2
[0023] Embodiment 2: The described core board is formed by pasting the particle core board and the reinforced bamboo chips on both sides, and the adhesive used includes 30 parts of ethylene-vinyl acetate copolymer, 35 parts of polyvinyl alcohol, 10 parts of acetamide, and 10 parts of joint agent, 6 parts of potassium persulfate, 8 parts of stearic acid, 2 parts of fiber magnesium silicate, 2 parts of toughening agent, and 5 parts of filler. The crosslinking agent is 1 / 2 zinc oxide and 1 / 2 lead oxide, the toughening agent is polysulfide rubber, and the filler is aluminum nitride. The preparation method of the adhesive only needs to mix and stir the above components.
Embodiment 3
[0024] Embodiment 3: The adhesive comprises 40 parts of ethylene-vinyl acetate copolymer, 30 parts of polyvinyl alcohol, 30 parts of acetamide, 8 parts of crosslinking agent, 8 parts of potassium persulfate, 5 parts of stearic acid, cellulose silicic acid Magnesium 5 parts, toughening agent 3 parts, filler 10 parts. The crosslinking agent is 1 / 3 lead oxide and 2 / 3 magnesium oxide, the toughening agent is nitrile rubber, and the filler is boron nitride.