Multifunctional metal surface composite treatment agent and preparation method and use method thereof
A composite treatment and metal surface technology, applied in the direction of metal material coating process, etc., can solve the problems of multiple treatment processes, labor protection problems, high cost, etc., to improve work efficiency, reduce labor costs and equipment costs, and high anti-corrosion performance effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0089] A multifunctional compound treatment agent for metal surfaces, comprising the following components in terms of mass percentage: water 44.70; manganese phosphate 10.00; magnesium chloride 10.00; sodium chloride 4.00; alkylbenzene sulfonate sodium 4.00; 10.00; Ethylene Glycol 1.00; Hydroxy Acid 2.00; Tartaric Acid 3.00; Methyl Acid 5.00;
Embodiment 2
[0091] A multifunctional composite treatment agent for metal surfaces, comprising the following components by mass percentage: 38.85% water; 9.00% manganese phosphate; 9.00% magnesium chloride; 5.00% sodium chloride; 5.00% sodium alkylbenzenesulfonate; 9.00; Ethylene Glycol 2.00; Hydroxy Acid 3.00; Tartaric Acid 5.00; Methyl Acid 6.00;
Embodiment 3
[0093] A multifunctional composite treatment agent for metal surfaces, comprising the following components by mass percentage: 42.75% water; 12.00% manganese phosphate; 12.00% magnesium chloride; 3.00% sodium chloride; 3.00% sodium alkylbenzenesulfonate; 8.00; Ethylene Glycol 1.50; Hydroxy Acid 2.00; Tartaric Acid 2.00; Methyl Acid 4.00;
[0094] A preparation method of a metal surface multifunctional composite treatment agent, comprising the steps of:
[0095] step one:
[0096] Add water, sodium alkylbenzene sulfonate, Pingpinga, vegetable tannin and ethylene glycol into the reaction tank, and rotate and stir steadily at normal temperature and pressure for 18 to 22 minutes; the best solution is 20 minutes.
[0097] Step two:
[0098] Then add manganese phosphate, hydroxy acid, tartaric acid and methyl acid into the reaction tank, and rotate and stir steadily at normal temperature and pressure for 22 to 28 minutes; the best solution is 25 minutes.
[0099] Step three:
[...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com