A composite powder and coating technology, applied in powder coatings, coatings and other directions, can solve problems such as inability to meet electrical spraying and surface protection, inability to meet production and living needs, poor physical properties, etc., to achieve good use prospects, cost reduction, The effect of wasting human resources
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A formula of composite powder coating, it is characterized in that, the formula of described composite powder coating comprises acrylic polyol resin 32%, curing agent 18%, auxiliary agent 3%, leveling agent 3%, barium sulfate 15% by weight percentage , titanium dioxide 6%, color masterbatch 2%, charge enhancer 3%, antioxidant 6% and anti-gas agent 12%, the sum of the quantities of each component is equal to 100%.
Embodiment 2
[0014] A formula for a composite powder coating, characterized in that, the formula of the composite powder coating comprises 37% of acrylic polyol resin, 19.5% of curing agent, 3% of auxiliary agent, 3% of leveling agent, and 12.5% of barium sulfate by weight percentage , titanium dioxide 5.5%, color masterbatch 2%, charge enhancer 3%, antioxidant 5.5% and anti-gas agent 9%, the sum of the quantities of each component is equal to 100%.
Embodiment 3
[0016] A formula for a composite powder coating, characterized in that, the formula of the composite powder coating comprises 42% of acrylic polyol resin, 21% of curing agent, 3% of auxiliary agent, 3% of leveling agent, and 10% of barium sulfate by weight percentage , titanium dioxide 5%, color masterbatch 2%, charge enhancer 3%, antioxidant 5% and anti-gas agent 6%, the sum of the quantities of each component is equal to 100%.
[0017] When preparing the composite paint formula of the present invention, each component batching is prepared according to the formula, put into a mixer, fully mix for 30min at a speed of 600 rpm, then put into a dryer to dry and form a sheet, and then pass The powder coating is obtained by grinding the powder with a pulverizer.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com