Fixation rosin ink

A technology of rosin and ink, applied in ink, household utensils, applications, etc., can solve the problem of poor color fixation of ink, achieve good color fixation effect, and help ink retention

Inactive Publication Date: 2017-06-20
南宁市青秀区嘉利林化有限公司
View PDF4 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] The technical problem to be solved by the present invention is to provide a color-fixing rosin ink to solve the problem that the color of the ink containing rosin components is not firmly fixed

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Fixation rosin ink
  • Fixation rosin ink

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0025] A color-fixing rosin ink, which is composed of the following components in parts by weight: 40 parts of epoxy resin, 30 parts of polymerized rosin, 15 parts of polyethylene glycol, 9 parts of Cuban gum, 1 part of sodium polyacrylic acid, dicyandiamide 3 parts of amine-formaldehyde polycondensate, 0.5 parts of black pigment.

[0026] The preparation method of described polymerized rosin is:

[0027] S1: Put 200g of industrial rosin in a three-necked flask, then add 1000mL of toluene, stir and heat to 75°C in an oil bath until the rosin is completely dissolved;

[0028] S2: Add 200g of concentrated sulfuric acid into the mixed solution obtained in step S1, heat for 40min, then add 20g of magnesium chloride and 10g of zinc chloride, heat to 120°C, and stir for 8h;

[0029] S3: filter the mixture obtained in step S2, wash the filtrate with deionized water at 85°C, and detect no chloride ions with silver chloride solution acidified with nitric acid;

[0030] S4: Take the f...

Embodiment 2

[0033] A color-fixing rosin ink, in parts by weight, consists of the following components: 115 parts of epoxy resin, 80 parts of polymerized rosin, 60 parts of polyethylene glycol, 22 parts of Cuban gum, 9 parts of polyvinyl alcohol, polydiene 15 parts of propyl dimethyl ammonium chloride, 2 parts of red pigment.

[0034] The preparation method of described polymerized rosin is:

[0035] S1: Put 200g of industrial rosin in a three-necked flask, then add 1000mL of toluene, stir and heat to 75°C in an oil bath until the rosin is completely dissolved;

[0036] S2: Add 200g of concentrated sulfuric acid into the mixed solution obtained in step S1, heat for 40min, then add 20g of magnesium chloride and 10g of zinc chloride, heat to 120°C, and stir for 8h;

[0037] S3: filter the mixture obtained in step S2, wash the filtrate with deionized water at 85°C, and detect no chloride ions with silver chloride solution acidified with nitric acid;

[0038] S4: Take the filtrate obtained i...

Embodiment 3

[0041] A color-fixing rosin ink, in parts by weight, consists of the following components: 45 parts of epoxy resin, 40 parts of polymerized rosin, 20 parts of polyethylene glycol, 11 parts of Cuban glue, 2 parts of polyacrylamide, dicyandiamide 5 parts of amine-formaldehyde polycondensate, 0.7 parts of pigment.

[0042] The preparation method of described polymerized rosin is:

[0043] S1: Put 200g of industrial rosin in a three-necked flask, then add 1000mL of toluene, stir and heat to 75°C in an oil bath until the rosin is completely dissolved;

[0044] S2: Add 200g of concentrated sulfuric acid into the mixed solution obtained in step S1, heat for 40min, then add 20g of magnesium chloride and 10g of zinc chloride, heat to 120°C, and stir for 8h;

[0045] S3: filter the mixture obtained in step S2, wash the filtrate with deionized water at 85°C, and detect no chloride ions with silver chloride solution acidified with nitric acid;

[0046] S4: Take the filtrate obtained in ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses fixation rosin ink and belongs to the technical field of ink. The fixation rosin ink comprises epoxy resin, polymeric rosin, polyethylene glycol, Cuban glue, a dispersant, a fixation agent and a pigment. The fixation rosin ink contains the fixation agent component and can effectively improve the fixation properties.

Description

technical field [0001] The invention belongs to the technical field of ink, and in particular relates to a color-fixing rosin ink. Background technique [0002] With the rapid development of the printing industry, consumers' requirements for the quality of printed matter are also increasing, and the quality of ink, which plays a key role in printing quality, is very important. Ink is a homogeneous mixture composed of colored bodies (such as pigments, dyes, etc.), linking materials, filling (filling) materials, additives, etc., and the additives (ie additives) are added to improve the printability of the ink. Such as viscosity, adhesiveness, dryness, etc. [0003] Rosin is a non-volatile natural resin obtained from pine rosin through different processing methods. Its main component is abietic (rosin) acid, which contains a carboxylic acid group and two conjugated carbon-carbon double bonds. It can be esterified with glycerin, pentaerythritol and other polyols to form low-ac...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D11/322C09D11/30C09D11/03C09D11/102C09D11/08
Inventor 谭伯堪陆文刚
Owner 南宁市青秀区嘉利林化有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products