A kind of lime-flue gas brine purification method

A brine purification and flue gas technology, applied in chemical instruments and methods, alkali metal chloride, water/sewage multi-stage treatment, etc., can solve the problems of strong caustic soda corrosion, lower pass rate, large amount of NaOH, etc., to achieve Low turbidity, stable flocculant, and the effect of reducing the cost of brine purification

Active Publication Date: 2018-03-20
JIANGXI JINGHAO SALINIZATION
View PDF3 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] The application and research of the two-alkali method in the deionization of salt-making brine is relatively mature. However, with the continuous rise of the market price of the two-alkali, the consumption of NaOH in the two-alkali method is large, the cost is high, and the caustic soda is highly corrosive. The loss is large, which also increases the production cost from another aspect
In addition, flocculants play a key role in the purification of brine. The existing flocculants cannot completely remove the suspended particles generated during the brine purification process, causing some suspended particles to enter the next process with the brine, and finally enter the salt products and nitrate products. The purity of the product is not high, or the qualified rate is reduced, and the annual loss is relatively large

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • A kind of lime-flue gas brine purification method

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0056] A method for purifying lime-flue gas brine, comprising the following steps:

[0057] 1) Primary reaction clarification: Sampling and analyzing the original halogen, measuring Ca in the original halogen 2+ , Mg 2+ Concentration, according to the amount of original halogen in the primary reaction barrel and the Ca in the original halogen 2+ , Mg 2+ Concentration value calculates the amount of required lime and soda ash, calculates the used reaction reaction equation as follows:

[0058] CaO+H 2 O→Ca(OH) 2

[0059] Ca(OH) 2 +Mg 2+ → Ca 2+ +Mg(OH) 2 ↓

[0060] Ca 2+ +Na 2 CO 3 →CaCO 3 ↓+2Na +

[0061] First, pump the original halogen into the primary reaction barrel, and at the same time, use 60% of the calculated lime amount to pre-feed lime into the primary reaction barrel. During the pre-feeding process, start the agitator in the primary reaction barrel to Stir so that the original brine and lime mix more evenly, stop feeding the original brine when the ...

Embodiment 2

[0074]A method for purifying lime-flue gas brine, comprising the following steps:

[0075] 1) Primary reaction clarification: Sampling and analyzing the original halogen, measuring Ca in the original halogen 2+ , Mg 2+ Concentration, according to the amount of original halogen in the primary reaction barrel and the Ca in the original halogen 2+ , Mg 2+ Calculating the amount of lime and soda ash required by the concentration value, first pump the original brine into the primary reaction tank, and at the same time use 70% of the calculated lime amount to pre-feed the lime into the primary reaction tank, and start during the pre-feeding process The agitator in the primary reaction tank stirs the original brine so that the original brine and lime can be mixed more evenly. When the liquid level of the original brine reaches the specified liquid level scale, stop feeding the original brine; then add the calculated amount of soda ash to the original brine Adding soda ash, the tim...

Embodiment 3

[0088] A method for purifying lime-flue gas brine, comprising the following steps:

[0089] 1) Primary reaction clarification: Sampling and analyzing the original halogen, measuring Ca in the original halogen 2+ , Mg 2+ Concentration, according to the amount of original halogen in the primary reaction barrel and the Ca in the original halogen 2+ , Mg 2+ Calculating the amount of lime and soda ash required by the concentration value, first pump the original brine into the primary reaction tank, and at the same time use 80% of the calculated lime amount to pre-feed the lime into the primary reaction tank, and start during the pre-feeding process The agitator in the primary reaction tank stirs the original brine so that the original brine and lime can be mixed more evenly. When the liquid level of the original brine reaches the specified liquid level scale, stop feeding the original brine; then add the calculated amount of soda ash to the original brine Adding soda ash, the ti...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
quality scoreaaaaaaaaaa
Login to view more

Abstract

The invention discloses a purification method of lime-flue gas brine, which comprises the following steps: 1) performing first-order reaction clarification: measuring concentration of Ca<2+> and Mg<2+> in raw brine, calculating required amount of lime and sodium carbonate, performing pre-feeding with the lime, feeding sodium carbonate to the raw brine and finally feeding the residual lime; 2) performing sampling and rework: testing concentration values of Ca<2+> and Mg<2+> in mixed brine liquid after a reaction, performing Step 3) if qualified, and performing further purification by utilizing caustic soda and sodium carbonate if unqualified; 3) performing primary flocculation: adding an HEC (Hydroxy Ethyl Cellulose)-maleic acid-chitosan composite flocculant to the mixed brine liquid for flocculating settling; 4) performing second-order reaction clarification: supplying carbon dioxide flue gas to liquid after the primary settling; 5) performing secondary flocculation: adding the HEC-maleic acid-chitosan composite flocculant to the brine liquid for the flocculating settling; 6) transferring liquid after the settling to a refined brine barrel of a salt manufacturing workshop. Compared with the traditional two-alkali method, the purification method has a great economic benefit; the composite flocculant is adopted, so that the purification time is short and the turbidity of the purified brine is low; the flocculant is more stable.

Description

technical field [0001] The invention relates to the technical field of salt making industry, in particular to a method for purifying lime-flue gas brine. Background technique [0002] As a necessity for human survival and one of the most basic raw materials for the chemical industry, salt plays a pivotal role in the daily life of the national economy. my country is one of the countries with the longest history of salt production in the world, and our country is rich in salt resources. Thousands of salt lakes are dotted in Qinghai, Xinjiang, Tibet and other provinces and autonomous regions. In Sichuan, Yunnan, Jiangsu, Shandong, Henan There are abundant mineral salt underground in Huai'an and other provinces, and Huai'an City has the largest salt mine in the world. [0003] Most of the brines of sulfate-type salt mines in my country contain Mg after water mining 2+ , Ca 2+ , SO 4 2- Due to the calcium and magnesium impurities contained in the brine, it is easy to precipit...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): C02F9/04C01D3/04
CPCC01D3/04
Inventor 林应南方远西周高峰刘钰林王乐
Owner JIANGXI JINGHAO SALINIZATION
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products