Papermaking method capable of improving paper quality
A quality and paper technology, applied in the field of papermaking to improve paper quality, can solve the problems of reducing the efficiency of dry strength agents and affecting the quality of paper products, and achieve the effect of maximizing the dosage of fillers, promoting bonding and reducing dosage.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A papermaking method for improving paper quality provided in this embodiment, the papermaking method for improving paper quality is specifically:
[0026] Step 1: adding the internally added starch to the milled slurry and sending it to the pipeline of the pulping tower, the dry pulp ratio of the internally added starch to the milled slurry is 14kg / t. When the liquid level of the slurry in the pulping tower is 45%, use the stirrer in the pulping tower to fully stir and mix the starch added in and the slurry after grinding, and then add flocculant in the pulping tower, the flocculant It has a reduced viscosity of 13 dL / g, a molecular weight of greater than or equal to 1,300,000 and less than or equal to 7,000,000, and a cationic charge of 35 mol%. Described step one per ton of packing, the consumption of described flocculant is 4kg. Using the agitator in the slurry forming tower to stir the above-mentioned mixture evenly to form the first mixed slurry, the particle size...
Embodiment 2
[0031] A papermaking method for improving paper quality provided in this embodiment, the papermaking method for improving paper quality is specifically:
[0032] Step 1: adding the internally added starch to the milled slurry and sending it to the pipeline of the pulping tower, the dry pulp ratio of the internally added starch to the milled slurry is 12kg / t. When the liquid level of the slurry in the pulping tower is 50%, use the agitator in the pulping tower to fully stir and mix the starch added in and the slurry after grinding, and then add flocculant in the pulping tower, the flocculant It has a reduced viscosity of 7 dL / g, a molecular weight of greater than or equal to 1,300,000 and less than or equal to 7,000,000, and a cationic charge of 40 mol%. In the step one, the amount of the flocculant is 0.2 kg per ton of filler. Using the agitator in the pulping tower to stir the above-mentioned mixture evenly to form the first mixed slurry, the particle size of the first mixed...
Embodiment 3
[0037] A papermaking method for improving paper quality provided in this embodiment, the papermaking method for improving paper quality is specifically:
[0038] Step 1: adding the internally added starch to the milled slurry and sending it to the pipeline of the pulping tower. The dry pulp ratio of the internally added starch to the milled slurry is 13kg / t. When the liquid level of the slurry in the pulping tower was 47%, use the stirrer in the pulping tower to fully stir and mix the starch added in and the slurry after grinding, and then add flocculant in the pulping tower, the flocculant It has a reduced viscosity of 9 dL / g, a molecular weight of greater than or equal to 1,300,000 and less than or equal to 7,000,000, and a cationic charge of 39 mol%. Described step one per ton of packing, the consumption of described flocculant is 2kg. Using the agitator in the slurry forming tower to stir the above-mentioned mixture evenly to form the first mixed slurry, the particle size...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com