A paint dyeing and polypropylene technology, which is applied in the field of textile auxiliaries, can solve the problems of poor stability of inorganic dispersants, inability to firmly adsorb particles, and unsatisfactory stability, and achieve extended service life, excellent gloss, and enhanced storage stability. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A preparation method of polyacrylic acid dispersant for paint dyeing, comprising the following steps:
[0022] (1) Epoxy cottonseed oil, acrylic acid, methacrylic acid, maleic acid, methylol acrylamide, emulsifier and water are added to the reaction kettle, after stirring evenly, take out half of the mixture emulsion for subsequent use;
[0023] (2) Add chain transfer agent and hydroxyethyl cellulose to the reactor, add sodium bicarbonate to adjust the pH to 5, stir and heat up to 80°C, and simultaneously dropwise add the aqueous solution of sodium persulfate and the solution taken out in step (1) Emulsion, stirring while adding dropwise, the stirring rate is 60rpm, continue to stir and react for 60min after the dropwise addition is completed, after cooling to room temperature, add NaOH to adjust the pH to 8, and concentrate by distillation under reduced pressure. After concentration under reduced pressure, the solid content is 60%. Prepare the polyacrylic acid dispersa...
Embodiment 2
[0027] A preparation method of polyacrylic acid dispersant for paint dyeing, comprising the following steps:
[0028] (1) Epoxy cottonseed oil, acrylic acid, methacrylic acid, maleic acid, methylol acrylamide, emulsifier and water are added to the reaction kettle, after stirring evenly, take out half of the mixture emulsion for subsequent use;
[0029] (2) Add chain transfer agent and hydroxyethyl cellulose to the reactor, add sodium bicarbonate to adjust the pH to 6, stir and heat up to 90°C, and simultaneously dropwise add the aqueous solution of sodium persulfate and the solution taken out in step (1) Emulsion, stirring while adding dropwise, the stirring rate is 90rpm, continue to stir and react for 90min after the dropwise addition is completed, after cooling to room temperature, add NaOH to adjust the pH to 9, vacuum distillation and concentration, the solid content after vacuum concentration is 70%, Prepare the polyacrylic acid dispersant for dyeing the paint.
[0030]...
Embodiment 3
[0033] A preparation method of polyacrylic acid dispersant for paint dyeing, comprising the following steps:
[0034] (1) Epoxy cottonseed oil, acrylic acid, methacrylic acid, maleic acid, methylol acrylamide, emulsifier and water are added to the reaction kettle, after stirring evenly, take out half of the mixture emulsion for subsequent use;
[0035] (2) Add chain transfer agent and hydroxyethyl cellulose to the reactor, add sodium bicarbonate to adjust the pH to 5, stir and heat up to 90°C, and simultaneously dropwise add the aqueous solution of sodium persulfate and the solution taken out in step (1) Emulsion, stirring while adding dropwise, the stirring rate is 60rpm, continue to stir and react for 90min after the dropwise addition is completed, after cooling to room temperature, add NaOH to adjust the pH to 8, and concentrate by distillation under reduced pressure. After concentration under reduced pressure, the solid content is 70%. Prepare the polyacrylic acid dispersa...