Embodiment 1
[0025] This embodiment relates to a new type of environmentally friendly paint, including the following raw materials in parts by weight: 10 parts of water-based alkyd resin, 20 parts of thermoplastic acrylic resin, 15 parts of amino resin, 8 parts of cobalt isooctanoate, 5 parts of pentaerythritol, 3 parts of dipropylene glycol butyl ether 5 parts of kaolin, 4 parts of nano-silver oxide, 3 parts of vegetable oily color paste, 6 parts of mica powder, 2 parts of zinc stearate, 5 parts of modified nano-diatomite, 0.8 parts of dispersant, 1 part of defoamer , 2 parts of thickener, 2 parts of film-forming aid, 15 parts of deionized water.
[0026] Wherein, the thickener is hydroxyethyl cellulose.
[0027] Wherein, the modified nano-diatomite is prepared by the following method: adding nano-diatomite to the sodium fatty acid solution, introducing carbon dioxide to adjust the pH of the solution to 5, controlling the reaction temperature to 100° C., and the reaction time to 25 minute...
Embodiment 2
[0038] This embodiment relates to a new type of environmentally friendly paint, including the following raw materials in parts by weight: 20 parts of water-based alkyd resin, 30 parts of thermoplastic acrylic resin, 25 parts of amino resin, 13 parts of cobalt isooctanoate, 10 parts of pentaerythritol, 7 parts of dipropylene glycol butyl ether 10 parts of kaolin, 6 parts of nano-silver oxide, 12 parts of vegetable oily color paste, 9 parts of mica powder, 4 parts of zinc stearate, 10 parts of modified nano-diatomite, 4 parts of dispersant, 2 parts of defoamer , 5 parts of thickener, 3 parts of film-forming aid, 25 parts of deionized water.
[0039] Wherein, the thickener is a montmorillonite clay thickener.
[0040] Wherein, the modified nano-diatomite is prepared by the following method: adding nano-diatomite to the sodium fatty acid solution, introducing carbon dioxide to adjust the pH of the solution to 6, controlling the reaction temperature to 110° C., and the reaction tim...
Embodiment 3
[0051] This embodiment relates to a new type of environmentally friendly paint, including the following raw materials in parts by weight: 14 parts of water-based alkyd resin, 23 parts of thermoplastic acrylic resin, 19 parts of amino resin, 10 parts of cobalt isooctanoate, 6 parts of pentaerythritol, 4 parts of dipropylene glycol butyl ether 7 parts of kaolin, 4.5 parts of nano-silver oxide, 7 parts of vegetable oily color paste, 7 parts of mica powder, 2.3 parts of zinc stearate, 7 parts of modified nano-diatomite, 1.5 parts of dispersant, 1.2 parts of defoamer , 3 parts of thickener, 2 parts of film-forming aid, 18 parts of deionized water.
[0052] Wherein, the thickener is hydroxyethyl cellulose.
[0053] Wherein, the modified nano-diatomite is prepared by the following method: adding nano-diatomite to the sodium fatty acid solution, introducing carbon dioxide to adjust the pH of the solution to 5.2, controlling the reaction temperature to 102° C., and the reaction time to...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com