A shock-absorbing rubber and automobile suspension technology, which is applied in the field of high-damping shock-absorbing rubber materials for automobile suspension bushings and its preparation, can solve the problems that rubber bushes cannot satisfy consumers well, and achieve enhanced anti-aging effects, Moderate degree of cross-linking and excellent overall performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] A high-damping shock-absorbing rubber material for automobile suspension bushings, the raw materials of which include by weight: 50 parts of methyl vinyl silicone rubber, 30 parts of polynorbornene rubber, 60 parts of nitrile rubber, and ionic liquid modified Ello 15 parts of stone, 20 parts of naphthenic oil, 10 parts of tackifying resin, 8 parts of zinc oxide, 20 parts of corn starch, 3 parts of paraffin, 2 parts of anti-aging agent, 1 part of vulcanizing agent, and 20 parts of processing aid.
Embodiment 2
[0026] A kind of high-damping shock-absorbing rubber material for automobile suspension bushing, its raw material comprises by weight: 70 parts of methyl vinyl silicone rubber, 20 parts of polynorbornene rubber, 100 parts of nitrile rubber, ionic liquid modified Ello 35 parts of stone, 40 parts of naphthenic oil, 15 parts of tackifying resin, 3 parts of zinc oxide, 10 parts of corn starch, 2 parts of paraffin, 2 parts of anti-aging agent, 5 parts of vulcanizing agent, and 8 parts of processing aid.
Embodiment 3
[0028] A high-damping shock-absorbing rubber material for automobile suspension bushings, the raw materials of which include by weight: 60 parts of methyl vinyl silicone rubber, 25 parts of polynorbornene rubber, 80 parts of nitrile rubber, and ionic liquid modified Ello 25 parts of stone, 30 parts of naphthenic oil, 12 parts of tackifying resin, 5 parts of zinc oxide, 15 parts of corn starch, 2.5 parts of paraffin, 1.5 parts of anti-aging agent, 3 parts of vulcanizing agent, and 15 parts of processing aid;
[0029] Wherein, the acrylonitrile content in the nitrile rubber is 31%;
[0030] The preparation process of ionic liquid-modified halloysite includes: weighing 3 parts of ionic liquid by weight and dispersing it in ethanol solution, adding 100 parts of halloysite, stirring evenly, ultrasonicating at 40°C for 1 hour, and drying to obtain ionic liquid Liquid modified halloysite.