A technology for optical glass and grinding fluid, applied in the field of grinding fluid, can solve the problems of affecting glass quality, poor lubricating performance, unfavorable cleaning, etc., and achieve the effects of improving surface quality, easy operation, and reducing grinding scratches
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] A kind of optical glass grinding liquid is prepared by following steps:
[0024] (1) 15 parts of tetradecyl dimethyl benzyl ammonium bromide, 15 parts of polyoxypropylene glycerol ether, 2 parts of polyethylene glycol fatty acid ester and 80 parts of water are added to the stirred reactor, and then Add 2 parts of n-propanolamine and 3 parts of isopropanolamine, stir until mixed evenly, and obtain the first mixed liquid;
[0025] (2) Heat the stirred reactor to 65°C, and keep stirring until the first mixed liquid in the kettle is transparent and uniform, then stop heating;
[0026] (3) Add 1 part of organosilicon defoamer into the stirred reactor, and then stir and mix evenly to obtain the optical glass grinding fluid.
Embodiment 2
[0028] A kind of optical glass grinding liquid is prepared by following steps:
[0029] (1) Add 5 parts of polydichloroethyl ether tetramethylethylenediamine, 20 parts of glycerol glycerol ether, 6 parts of polyethylene glycol fatty acid ester and 90 parts of water into the stirred reactor, and then add N - 1 part of methyldiethanolamine, stirred until uniformly mixed to obtain the first mixed solution;
[0030] (2) Heat the stirred reactor to 60°C, and keep stirring until the first mixed liquid in the kettle is transparent and uniform, then stop heating;
[0031] (3) Add 3 parts of organosilicon defoamer into the stirred reactor, and then stir and mix evenly to obtain the optical glass grinding fluid.
Embodiment 3
[0033] A kind of optical glass grinding liquid is prepared by following steps:
[0034] (1) Add 10 parts of polyoxyethylene lauryl dimethyl ammonium bromide, 5 parts of polyoxyethylene glycerol ether, 10 parts of polyethylene glycol and 100 parts of water into the stirred reactor, and then add isopropyl Alcoholamine 2 and 2 parts of ethylenediamine, stirred until uniformly mixed to obtain the first mixed solution;
[0035] (2) Heat the stirring reaction kettle to 70°C, and keep stirring until the first mixed liquid in the kettle is transparent and uniform, then stop heating;
[0036] (3) Add 5 parts of organosilicon defoamer into the stirred reactor, and then stir and mix evenly to obtain the optical glass grinding fluid.