A multifunctional concrete technology, applied in the field of construction, can solve the problems of concrete use function and occasion limitation, concrete function singleness, etc., achieve good hydrophobicity and self-cleaning characteristics, rich functional diversity, and reduce dust pollution.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A multifunctional building concrete, comprising the following components in parts by weight: 10 parts of phosphorus slag, 5 parts of fly ash, 3 parts of cement, 3 parts of PDMS, 1 part of straw ash, 3 parts of nickel powder, and 1 part of chromium powder 1 part, 2 parts of aluminum oxide powder, 1 part of silicon carbide powder, 3 parts of lime powder, 1 part of asbestos, 1 part of glass fiber, 1 part of silicon micropowder, 0.2 part of stearyl mercaptan.
[0023] The construction method of a kind of multifunctional building concrete as described above comprises the following manufacturing steps:
[0024] (1) Take the following components in parts by weight: 3 parts of PDMS, 1 part of silicon carbide powder, 1 part of asbestos, 0.2 parts of stearyl mercaptan; first mix the silicon carbide powder and asbestos evenly, and then mix the liquid PDMS Uniformly coated on the surface of silicon carbide powder and asbestos mixture, after stirring for 10 minutes, add stearyl merc...
Embodiment 2
[0033] A multifunctional building concrete, comprising the following components in parts by weight: 12 parts of phosphorus slag, 7 parts of fly ash, 5 parts of cement, 5 parts of PDMS, 2 parts of straw ash, 5 parts of nickel powder, and 2 parts of chromium powder 5 parts, 5 parts of aluminum oxide powder, 2 parts of silicon carbide powder, 5 parts of lime powder, 2 parts of asbestos, 2 parts of glass fiber, 2 parts of silicon micropowder, 0.5 part of stearyl mercaptan.
[0034] The construction method of a kind of multifunctional building concrete as described above comprises the following manufacturing steps:
[0035] (1) Take the following components in parts by weight: 5 parts of PDMS, 2 parts of silicon carbide powder, 2 parts of asbestos, and 0.5 parts of stearyl mercaptan; first mix the silicon carbide powder and asbestos evenly, and then mix the liquid PDMS Evenly coat the surface of the silicon carbide powder and asbestos mixture, stir for 15 minutes, then add stearyl ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com