Large blast furnace mixed injection meager lean coal application method
An application method and technology of lean and lean coal, applied in the field of smelting, can solve the problems of insufficient supply, low resource reserves of high-quality anthracite coal, and rising price of anthracite, so as to reduce production costs, obtain social environmental protection benefits, and reduce environmental pollution.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0014] A method for applying mixed injection of lean coal in a large blast furnace. The ratio of anthracite, bituminous coal and lean coal is: anthracite: bituminous coal: lean coal = 70-72:10-12:20-21;
[0015] Bituminous coal has a carbon content of 75%-90%, a density of 1.2-1.5, and a volatile matter of about 10%-40%. Relative density 1.25~1.35, calorific value 27170-37200 kJ / kg (6500-8900 kcal / kg);
[0016] Anthracite has a carbon content of more than 90%, a volatile matter of less than 10%, and no colloidal layer thickness. The calorific value is about 6000-6500 kcal / kg.
[0017] The indicators of lean coal are as follows, 5500 kcal, moisture less than 6, volatile content 12-18, sulfur content less than 1.5.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com