A glove and soft technology, applied in the field of knitting gloves, can solve problems such as easy to break fingers, reduce the quality of knitting products, and unfavorable strength, so as to enhance processing performance and anti-slip performance, avoid soaking feeling and the growth of germs, and enhance communication. The effect of coupling ability and wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A wear-resistant, soft and skin-friendly woven glove, made of the following raw materials in parts by weight: modified butadiene rubber 62, latex 21, polyamide fiber 46, medical stone fiber 13, graphene fiber 7, polyvinyl alcohol 6. Modified styrene-acrylic emulsion14.
[0021] For the modified butadiene rubber, add butadiene rubber into ethyl acetate with 1.6 times the weight of butadiene rubber, heat to 65°C at a speed of 0.5°C / min, stir evenly, add borax solution, mix evenly, and Continue to heat up to 80°C at a speed of 1.1°C / min, keep stirring for 2 hours, and freeze-dry until there is no moisture to obtain modified butadiene rubber, which enhances the processing performance and anti-skid performance of butadiene rubber.
[0022] Described borax solution, mass percent concentration is 2.3%, and adding volume is 3.4 times of ethyl acetate volume.
[0023] For the modified styrene-acrylic emulsion, heat the styrene-acrylic emulsion to 60°C at a rate of 0.6°C / min, ad...
Embodiment 2
[0031] A wear-resistant, soft and skin-friendly woven glove, made of the following raw materials in parts by weight: modified butadiene rubber 63, latex 22, polyamide fiber 47, medical stone fiber 14, graphene fiber 8, polyvinyl alcohol 7. Modified styrene-acrylic emulsion 15.
[0032] For the modified butadiene rubber, add butadiene rubber into ethyl acetate with 1.7 times the weight of butadiene rubber, heat to 68°C at a speed of 0.6°C / min, stir evenly, add borax solution, mix evenly, and Continue to heat up to 83°C at a speed of 1.2°C / min, keep stirring for 2.5 hours, and freeze-dry until there is no moisture to obtain modified butadiene rubber, which enhances the processing performance and anti-skid performance of butadiene rubber.
[0033] Described borax solution, mass percentage concentration is 2.4%, and adding volume is 3.5 times of ethyl acetate volume.
[0034] For the modified styrene-acrylic emulsion, heat the styrene-acrylic emulsion to 63°C at a rate of 0.7°C / m...
Embodiment 3
[0042] A wear-resistant, soft and skin-friendly woven glove, made of the following raw materials in parts by weight: modified butadiene rubber 64, latex 23, polyamide fiber 48, medical stone fiber 15, graphene fiber 9, polyvinyl alcohol 8. Modified styrene-acrylic emulsion 16.
[0043] For the modified butadiene rubber, the butadiene rubber is added to ethyl acetate of 1.8 times the weight of the butadiene rubber, heated to 70°C at a speed of 0.7°C / min, stirred evenly, added borax solution, mixed evenly, and Continue to heat up to 85°C at a speed of 1.3°C / min, keep stirring for 3 hours, and freeze-dry until there is no moisture to obtain modified butadiene rubber, which enhances the processing performance and anti-skid performance of butadiene rubber.
[0044] Described borax solution, mass percentage concentration is 2.5%, and adding volume is 3.6 times of ethyl acetate volume.
[0045] For the modified styrene-acrylic emulsion, heat the styrene-acrylic emulsion to 65°C at a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com