Complex iron preparation and preparation method thereof
A technology of complexing iron and organic complexing agents, which is applied in the direction of separation methods, chemical instruments and methods, gas fuels, etc., can solve the problems of high regeneration air consumption, slow regeneration rate, and low sulfur capacity, so as to reduce air consumption, The effect of accelerating regeneration rate and reducing regeneration energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] Hydroxyethylethylenediaminetriacetic acid (HEDTA), KOH, FeCl 2 ·H 2 O, CoCl 2 ·6H 2 O was mixed with water, the mass percentage of iron ions was 7wt%, the molar ratio of Co / Fe was 0.1, the molar ratio of HEDTA / (Fe+Co) was 3.0, the molar ratio of KOH / Fe was 1.2, and the mixing time was 5h at room temperature.
[0032] Air was introduced sequentially for 3.5 hours; 7wt% piperazine was added, and it was fully stirred evenly; then 2wt% polyethylene glycol (molecular weight was 600) was added, and it was fully stirred evenly for 1.5h to obtain the complex Iron preparations.
Embodiment 2
[0037] Hydroxyethylenediaminetetraacetic acid (EDTA), NaOH, FeSO 4 ·7H 2 O. CoSO 4 ·7H 2 Mix O and water, the mass percentage of iron ion is 0.5wt%, the molar ratio of Co / Fe is 0.01, the molar ratio of EDTA / (Fe+Co) is 1.2, the molar ratio of NaOH / Fe is 0.8, and the mixing time is 3h at room temperature .
[0038] Air was introduced sequentially for 2.5 hours; 1wt% piperazine was added, and it was fully stirred evenly; then 0.1wt% polyethylene glycol (molecular weight was 400) was added, and it was fully stirred evenly for 1 hour to obtain the complex Iron preparations.
Embodiment 3
[0043] Diethylenetriaminepentacic acid (DTPA), NaOH, Fe(C 4 h 6 o 4 ) 3 、CoCl 2 ·6H 2 O and water were mixed, the mass percentage of iron ions was 7wt%, the molar ratio of Co / Fe was 0.02, the molar ratio of DTPA / (Fe+Co) was 2.5, the molar ratio of NaOH / Fe was 1.0, and the mixing time was 3h at room temperature.
[0044] Air was introduced sequentially for 3.0 hours; 3wt% piperazine was added, and it was fully stirred evenly; then 0.8wt% polyethylene glycol (molecular weight: 2000) was added, and it was fully stirred evenly for 1 hour to obtain the complex Iron preparations.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com