Cleaning agent and preparation method thereof
A technology of cleaning agent and emulsifier, which is applied in the field of cleaning agent for cleaning synthetic resin reactors and its preparation, and can solve problems such as difficult cleaning of synthetic resin reactors
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0042] Another embodiment of the present invention provides a method for preparing the above cleaning agent, which specifically includes the following steps:
[0043] According to the raw material formula of the cleaning agent, the emulsifier and the water-soluble polymer are added to the water, and the emulsifier and the water-soluble polymer are stirred until the emulsifier and the water-soluble polymer are dissolved to obtain the first mixture;
[0044] Adding a pH adjuster to the first mixture, and continuing to stir until uniformly mixed, to obtain a second mixture;
[0045] Add an organic solvent into the second mixture and mix well to obtain a cleaning agent.
[0046] In this way, strictly controlling the order in which each component is added to the water can ensure that the components are fully dissolved and mixed with each other, so as to avoid affecting the use of the cleaning agent due to insoluble or insoluble components.
[0047] It can be understood that the mi...
Embodiment 1
[0053] 1) A formula of cleaning agent: 35 parts of water + 30 parts of organic solvent + 3 parts of emulsifier + 0.8 parts of water-soluble polymer + 6 parts of pH regulator.
[0054] 2) Preparation method:
[0055] Accurately weigh 35.0 kg of tap water and put it into the stainless steel dispersion tank. Under the condition of stirring (butterfly stirring), weigh 3.0 kg of emulsifier Tween-20 and add it to the dispersion tank, and weigh 0.8 kg of water-soluble polymer PVA-1788 Add to the dispersion tank, stir at low speed until the emulsifier and high molecular polymer are completely dissolved, then add 6.0 kg of pH regulator sodium carbonate, stir at low speed to dissolve, add 30.0 kg of ethyl ester organic solvent, stir well and pack for later use.
[0056] The obtained cleaning agent is a translucent viscous liquid, and the measured viscosity of the cleaning agent is 11000 centipoise and the pH value is 10.8.
Embodiment 2
[0058] 1) A formula of cleaning agent: 50 parts of water + 25 parts of organic solvent + 3.5 parts of emulsifier + 0.5 parts of water-soluble polymer + 3 parts of pH regulator.
[0059] 2) Preparation method:
[0060] Accurately weigh 50.0 kg of tap water and put it into the stainless steel dispersing tank. Under the condition of stirring, weigh 3.5 kg of emulsifier isomerized thirteen polyoxyethylene ether (E-1320) and add it to the dispersing tank. Add 0.5 kg of acrylamide to the dispersing tank, stir at low speed until the emulsifier and high molecular polymer are completely dissolved, then add 3.0 kg of sodium hydroxide pH regulator, stir at low speed to dissolve, add 25.0 kg of acetone organic solvent, stir well and pack for later use.
[0061] The obtained cleaning agent is a translucent viscous liquid, and the measured viscosity of the cleaning agent is 10500 centipoise and the pH value is 11.6.